One of the problems encountered in 60′s to 80′s of 20th century in China′s steel industry was short life of blast furnace shaft as well as the excessive erosion of blast furnace hearth. A series of research work was carried out in order to extend blast furnace campaign life. The concept of research and development was integrated in the construction of BF (blast furnace) No5 at WISCO (Wuhan Iron and Steel Corporation), and in October, 1991, the BF No5 was blown in. The blast furnace has worked smoothly for more than 15 years without any medium repair even guniting. It is expected that the campaign life of BF No5 would be longer than 16 years with a production over 11 000 t per unit inner volume (m3). A new blast furnace with an inner volume of 3 400 m3 is under construction, and is designed with a campaign life of 20 years without any medium repair. The campaign life of blast furnaces in China has been extended in recent years.
关键词:
blast furnace;campaign life;erosion
Journal of Materials Research
The morphology of the dark and bright regions observed by transmission electron microscopy for the Zr(64.13)Cu(15.75)Ni(10.12)Al(10) bulk metallic glass strongly depends on the ion beam parameters used for ion milling. This indicates that the ion beam could introduce surface fluctuation to metallic glasses during ion milling.
关键词:
room-temperature
Philosophical Magazine
The error of Equation (15b) in my article [Z.D. Zhang, Phil. Mag. 87 (2007) p.5309] in the application of the Jordan-Wigner transformation does not affect the validity of the putative exact solution, since the solution is not derived directly from that equation. Other objections of Perk's comment [J.H.H. Perk, Phil. Mag. 89 (2009) p.761] are the same as those in Wu et al.'s comments [F.Y. Wu et al., Phil. Mag. 88 (2008) p.3093; p.3103], which do not stand on solid ground and which I have sought to refute in my previous response [Z.D. Zhang, Phil. Mag. 88 (2008) p.3097]. The conjectured solution can be utilized to understand critical phenomena in various systems, whereas the conjectures are open to rigorous proof.
关键词:
3D Ising model;exact solution;conjecture;critical phenomena;ferromagnetism;magnetic phase transition;model;analyticity
中国腐蚀与防护学报
N。1Atmospheric Corrosivlty for Steels………………………………………………… .LIANG Caideng HO[I i。-tat(6)Caustic Stress Corrosion Cr。king of Alloy 800 Part 2.The Effect of Thiosul执e……………………………………… KONG De-sheng YANG Wu ZHAO Guo-zheng HUANG De.ltL。ZHANG Yu。。he CHEN She。g-bac(13)SERS slid E16CttOCh6iniC81 Stlldy Of Illhibit1Oli M6ch&tllsth Of ThlollY68 Oil ITOll ID H....
关键词:
Physics Letters A
In a magnetic system, consistent with Griffiths analyticity requirements one can parameterize the equation of state near criticality by writing H = r(beta delta)h(theta), T = rt(theta) and the magnetization M = r(beta)m(theta), where T is measured from the critical temperature. For the insulating ferromagnet CrBr(3), the experimental data of Ho and Litster [J.T. Ho, J.D. Litster, Phys. Rev. Lett. 22 (1969) 6031 is well fitted by m(theta) as a linear function of theta [P. Schofield, J.D. Litster, J.T Ho, Phys. Rev. Lett. 23 (1969) 1098]. Also Ho and Litster give beta = 0.368, gamma = 1.215 and delta = 4.3. Those critical experiments are very close to the recent 31) king results of Zhang [Z.D. Zhang, Philos. Mag. 87 (2007) 5309], namely beta = 3/8, gamma = 5/4 and delta = 13/3. We therefore predict that m(theta) will be proportional to theta as a fingerprint of the 3D Ising Hamiltonian. (C) 2009 Elsevier B.V. All rights reserved.
关键词:
Critical-point effects;Critical exponents;Ising model;Criticality;Ferromagnet;Magnetic equation of state;critical exponents
刘守平
,
周上祺
,
王佳眉
,
任勤
腐蚀学报(英文)
用金相显微镜、扫描电镜、X射线衍射仪和X射线能谱仪对天然气井油管悬挂器腐蚀失效进行了检测分析,并对天然气井油管悬挂器用35CrMo钢进行了盐雾试验,结果表明,天然气中的水和CO2是引起腐蚀的主要介质,腐蚀产物主要是FeCO3,高速天然气冲刷和钢中的非金属夹杂加剧了腐蚀的速度.
CORROSION FAILURE ANALYSIS OF AN OIL TUBE USED IN NATURAL GAS WELL
LIU Shou-ping,ZHOU Shang-qi,WANG Jia-mei,REN Qin
Chongqing University
A failed oil tube used in natural gas well was examined by optical microscope,scanning electron microscope ,X-ray diffractometer and X-ray spectrometer.Corrosion behavior of 35CrMo steel samples of the oil tube were investigated by means of salt spray tests in the laboratory.The results show that CO2 and H2O are primary factors in the corrosion of oil tube.The corrosion product is FeCO3,non-metallic inclusions in the steel and erosion of natural gas fluid played an important role in accelerating the corrosion.
oil tube;
natural gas well;
35CrMo steel;
failure analysis;
corrosion