THERMODYNAMICS OF V REDUCTION IN SMELTING REDUCTION SLAG FOR V-Ti-CONTAINING MAGNETITE

ZHANG Binhuai LIU Qingcai LI Changwei ZOU Deyu SUN Jinbiao Chongqing University , Chongqing , China professor , Department of Metallurgy and Materials Engineering , Chongqing University , Chongqing 630044 , China

金属学报(英文版)

For slag system of CaO-SiO_2-Al_2O_3-MgO-V_2O_5,the time of V reduction to appro ch the dynamical equilibrium is about 6 h,the equilibrium time is not evidently influenced by the ratio CaO/SiO_2 and shortens with the increase of temperature.It the ratio of the weight of slag to that of iron bath is 1/2,CaO/SiO_2 0.8 and tomperature 1773 K.the maxium distribution coefficeent of V reduction is 32.4 and maxium recovery of V is 96.1%.

关键词: magnetite , null , null , null

天然气井油管悬挂器腐蚀失效分析

刘守平 , 周上祺 , 王佳眉 , 任勤

腐蚀学报(英文)

用金相显微镜、扫描电镜、X射线衍射仪和X射线能谱仪对天然气井油管悬挂器腐蚀失效进行了检测分析,并对天然气井油管悬挂器用35CrMo钢进行了盐雾试验,结果表明,天然气中的水和CO2是引起腐蚀的主要介质,腐蚀产物主要是FeCO3,高速天然气冲刷和钢中的非金属夹杂加剧了腐蚀的速度. CORROSION FAILURE ANALYSIS OF AN OIL TUBE USED IN NATURAL GAS WELL LIU Shou-ping,ZHOU Shang-qi,WANG Jia-mei,REN Qin Chongqing University A failed oil tube used in natural gas well was examined by optical microscope,scanning electron microscope ,X-ray diffractometer and X-ray spectrometer.Corrosion behavior of 35CrMo steel samples of the oil tube were investigated by means of salt spray tests in the laboratory.The results show that CO2 and H2O are primary factors in the corrosion of oil tube.The corrosion product is FeCO3,non-metallic inclusions in the steel and erosion of natural gas fluid played an important role in accelerating the corrosion. oil tube; natural gas well; 35CrMo steel; failure analysis; corrosion

关键词: 悬挂器 , null , null , null

ON SPINODAL BOUNDARIES OF Al-Li ALLOYS

WEI Yinghui , WANG Xiaotian (School of Materials Scince and Engineering , Xi'an Jiaotong University , Xi'an 710049 , China Manuscript received 10 Mareh , 1994)

金属学报(英文版)

The spinodal decomposition can occur in Al-Li alloys containing 5.8-14.2 at.% Li at room temperature. The modutated structure wavelength is approximately 3.1 nm for com mercial Al-LI alloys. The limit composition of the miscibility gap is 3.66 -16.06 at.%Li at 298 K. The highest temperature of the miscibility gap is 377 K.

关键词: : Al-Li alloy , null , null

大爆炸核合成相关的8Li(d, p)9Li反应截面测量

李志宏 , 柳卫平 , 白希祥 , 郭冰 , 连钢 , 颜胜权 , 王宝祥 , 陆昀 , 曾晟 , 苏俊

原子核物理评论 doi:10.3969/j.issn.1007-4627.2005.01.006

利用8Li次级束测量了质心系能量7.8 MeV 2H(8Li, 9Li)1H反应的角分布, 导出了8Li(d, p)9Li反应的天体物理S因子及9Li→8Li+n虚衰变的渐近归一化系数.

关键词: 8Li(d,p)9Li反应 , 角分布 , 天体物理S因子 , 渐近归一化系数

CRYSTAL STRUCTURE OF γ-Li_xFe_2O_3 WITH ELECTROCHEMICAL INSERTION OF Li

HUANG Jianshun CHEN Junming Shanghai Institute of Metallurgy , Academia Sinica , Shanghai , China Research Associate , Shanghai Institute of Metallurgy , Academia Sinica , Shanghai 200050 , China

金属学报(英文版)

Crystal structure of γ-Li_xFe_2O_3,inserted Li electrochemically,was studied by Moss- bauer spectroscopy together with X-ray diffraction,XPS and electrochemical method,On the insertion of Li at low current density,the crystal structure is keeping original spinel; while at higher current density or by thermal activation,owing to violent movement of Li~+ ions,part of crystal structure transforms into rock type similar to face-centered cubic structure of ferrous oxide.The transition channels during insertion of Li~+ ions and limitation of Li~+ ions inserted were discussed.