ZHAO Shu-mao
,
MEI Guo-hui
,
XIE Zhi
钢铁研究学报(英文版)
MgO-C continuous temperature-measuring sensors for liquid steel were made of fused magnesia with different critical particle sizes from 05 to 20 mm, thus the effects what magnesia′s particle size affect sensors′ properties and lifetime were studied. The result shows that the MgO-C continuous temperature-measuring sensor has good aggression resistance to basic tundish powders and meets the requirement for response time of temperature measuring practice in tundish. The sensor′s service life, which is affected by multi-properties of material and operating environment, reached its maximum when the critical particle size of magnesia was 10 mm. The average lifetime of sensors was 43 or 40 h when served for casting SPHC or Q195 steel.
关键词:
MgO
,
carbon
,
microstructure
,
sensors
,
lifetime
,
particle size
马乾志
,
郭杨龙
,
王艳芹
,
郭耘
,
张志刚
,
卢冠忠
无机材料学报
doi:10.3321/j.issn:1000-324x.2007.05.033
采用TS-1前驱体作硅源和钛源,以十二胺为模板剂,在中性和室温条件下合成了介孔含钛分子筛Ti-HMS-1.采用XRD、TEM、低温N2吸附、FT-IR和UV-Vis等方法对合成的分子筛进行了表征;以苯乙烯的催化氧化反应为模型反应,考察了合成的Ti-HMS-1的催化氧化性能.结果表明,Ti-HMS-1具有"worm-like"介孔结构,但长程有序度较低,孔壁部分含有MFI的次级结构单元,在373K沸水中水煮50h后,Ti-HMS-1仍能较好地保持原有的介孔结构,表明Ti-HMS-1具有较高的水热稳定性.进入分子筛骨架的钛原子为催化剂的活性中心,对于苯乙烯氧化反应,具有较高的催化活性,对产物的选择性与Ti-HMS接近.
关键词:
Ti-HMS-1分子筛
,
合成
,
表征
,
苯乙烯氧化
周萧明
,
胡更开
复合材料学报
doi:10.3321/j.issn:1000-3851.2004.06.026
提出了预测复合材料非线性电位移和电场强度关系的一种解析方法,该方法基于各向材料的割线介电常数,将非线性问题转化成一系列线性问题来求解.该方法适用于任意各向异性复合材料和组分材料的非线性性质,而常用的Stroud和Hui的模型只适用于各向同性复合材料和组分材料的弱线性.证明了本文方法具有Ponte Castaneda提出的变分结构.计算结果表明,当基体非线性较小时,本文模型的预测与Stroud和Hui的模型一致,但当基体非线性系数增大时,本文模型能给出合理的预测结果,而Stroud和Hui的模型则会超出基体和夹杂的性能范围.
关键词:
复合材料
,
介电常数
,
非线性
,
割线方法
Journal of Chemical Physics
Based on Mei's embedded atom model [Mei , Phys. Rev. B 43, 4653 (1991)] molecular dynamics simulations have been performed to investigate the rapidly cooling processes of Cu. The atomic transport property, namely the self-diffusion coefficient, is computed in the liquid state, and the results near the melting point of Cu are in good agreement with experimental data and other computational values. The atom diffusion movements during the long period of relaxation have been also studied around the solidification temperature T-c. To describe the complex microstructural evolutions during the rapidly cooling processes and the long relaxation processes, the pair correlation function and the pair analysis technique are used. It is demonstrated that the crystallization of amorphous Cu is caused by the atomic diffusion. (C) 2004 American Institute of Physics.
关键词:
transition-metals;computer-simulation;supercooled-liquid;model;fcc;potentials;diffusion
中国腐蚀与防护学报
N。1Atmospheric Corrosivlty for Steels………………………………………………… .LIANG Caideng HO[I i。-tat(6)Caustic Stress Corrosion Cr。king of Alloy 800 Part 2.The Effect of Thiosul执e……………………………………… KONG De-sheng YANG Wu ZHAO Guo-zheng HUANG De.ltL。ZHANG Yu。。he CHEN She。g-bac(13)SERS slid E16CttOCh6iniC81 Stlldy Of Illhibit1Oli M6ch&tllsth Of ThlollY68 Oil ITOll ID H....
关键词:
刘守平
,
周上祺
,
王佳眉
,
任勤
腐蚀学报(英文)
用金相显微镜、扫描电镜、X射线衍射仪和X射线能谱仪对天然气井油管悬挂器腐蚀失效进行了检测分析,并对天然气井油管悬挂器用35CrMo钢进行了盐雾试验,结果表明,天然气中的水和CO2是引起腐蚀的主要介质,腐蚀产物主要是FeCO3,高速天然气冲刷和钢中的非金属夹杂加剧了腐蚀的速度.
CORROSION FAILURE ANALYSIS OF AN OIL TUBE USED IN NATURAL GAS WELL
LIU Shou-ping,ZHOU Shang-qi,WANG Jia-mei,REN Qin
Chongqing University
A failed oil tube used in natural gas well was examined by optical microscope,scanning electron microscope ,X-ray diffractometer and X-ray spectrometer.Corrosion behavior of 35CrMo steel samples of the oil tube were investigated by means of salt spray tests in the laboratory.The results show that CO2 and H2O are primary factors in the corrosion of oil tube.The corrosion product is FeCO3,non-metallic inclusions in the steel and erosion of natural gas fluid played an important role in accelerating the corrosion.
oil tube;
natural gas well;
35CrMo steel;
failure analysis;
corrosion
关键词:
悬挂器
,
null
,
null
,
null
李凤娟
,
吕国光
金属世界
doi:10.3969/j.issn.1000-6826.2014.04.14
通过对烧结配料所需原料及对冷烧结矿成品检验采制样方法的分析,找出影响检验结果真实性的因素,采取有效的改进措施,使本钢原料厂一次配料、本钢炼铁厂265 m2烧结二次配料及265 m2烧结系统各项稳定率有了很大的提高,烧结矿实物质量和各项技术质量指标有了很大的进步,保证了高炉的稳定顺行。
提高本钢265 m2冷烧结矿及原料检验代表性的实践
Practice of Improving the 265 m2 Cold Sinter and Raw Material Inspection Representative
供稿|
李凤娟,吕国光/
LI Feng-juan, LV Guo-guang
DOI:10.3969/j.issn.1000-6826.2014.04.14
导读内容
本钢炼铁厂265 m2烧结机生产所需要的含铁原料比较复杂,一次配料料种较多,且烧结含铁原料是由本钢原料厂二车间供料,原料质量的不稳定,会影响烧结矿质量的提高和新一号高炉的强化及高炉技术指标的改善。本钢质量管理中心驻冷烧检查站加强了对烧结配料所需原料及对冷烧结矿成品检验采制样代表性的研究,采取了一些改进措施,达到了良好的效果。含铁料成分稳定率、烧结矿各项质量和技术指标在稳步地提高。下面,对本钢质量管理中心驻冷烧检查站就提高采样及检验过程的准确性所采取的措施和办法进行说明。
烧结矿采样是半自动采样,每两小时采样一次,作为一个批次,来代表整个2h烧结矿的成份。
关键词: