Guofeng Wang Kaifeng Zhang
材料科学技术(英文)
Ni-Mn nanocomposite reinforced by Al2O3 particles was fabricated by pulse electrodeposition. The average grain size is 60 nm and the content of Mn and Al2O3 particles is 0.3 and 0.6 wt pct, respectively. The superplastic deformation behavior was further studied at the temperatures ranging from 673 to 873 K. A maximum elongation of 530% is obtained in the tension test at a temperature of 773 K and at a strain rate of 1.67×10-3 s-1. The curves of the flow stress vs strain rate have features similar to the trend of conventional superplastic materials. The test temperature (773 K) equals to 0.35Tm, which means the material obtains low temperature superplasticity. The microstructures of the composite were examined and grain growth was observed during deformation.
关键词:
Electrodeposition
,
纳米复合材料
,
低温超塑性
,
显微组织
YU Yuanhao
,
FENG Gensheng
,
SU Dongxue
钢铁研究学报(英文版)
To further decrease the fuel consumption of blast furnace in Tangshan Guofeng Iron and Steel Co Ltd, measures of improving the quality of sinter and pellet and the performances of raw materials were put forward through phase analysis and physical and chemical performance testing. The measures of increasing the grade of sinter, decreasing the sinter reduction degradation index at low temperature, and increasing the sinter soft melt performance at elevated temperature, as well as the reasonable process parameters of sintering were described in detail.
关键词:
sinter;metallurgical property;process parameter
Journal of Materials Research
The morphology of the dark and bright regions observed by transmission electron microscopy for the Zr(64.13)Cu(15.75)Ni(10.12)Al(10) bulk metallic glass strongly depends on the ion beam parameters used for ion milling. This indicates that the ion beam could introduce surface fluctuation to metallic glasses during ion milling.
关键词:
room-temperature
Journal of Physics and Chemistry of Solids
The layered ternary ceramics Ti3SiC2 and Ti3AlC2 are isostructural and can form Ti3Si1-xAlxC2 solid solutions combining the advanced properties of both compounds [H.B. Zhang, Y.C. Zhou, Y.W. Bao, M.S. Li, Improving the oxidation resistance of Ti3SiC2 by forming a Ti3Si0.90Al0.1C2 solid solution, Acta Mater. 52 (2004) 3631-3637; E.D. Wu, J.Y. Wang, H.B. Zhang, Y.C. Zhou, K. Sun, Y.J. Xue, Neutron diffraction studies of Ti3Si0.9Al0.1C2 compound, Mater. Lett. 59 (2005) 2715-2719; J.Y. Wang, Y.C. Zhou, First-principles study of equilibrium properties and electronic structure of Ti3Si0.75Al0.25C2 solid solution, J. Phys.: Condens. Matter 15 (2003) 5959-5968; Y.C. Zhou, J.X. Chen, J.Y. Wang, Strengthening of Ti3AlC2 by incorporation of Si to form Ti3Al1-xSixC2 solid solutions, Acta. Mater. 54 (2006) 1317-1322]. In the present work, the solid solutions of Ti3Si1-xAlxC2 (x = 0, 0.25, 0.33, 0.5, 0.67, 0.75, 1) are investigated by first-principle calculations based on pseudo-potential plan-wave method within the density functional theory framework. The results show that as Al content increases in the solid solution, all the bonds have weakened to certain extents, which lead to an unstable structure both energetically and geometrically. The calculated results are compared and discussed with the reported data for the Ti3Si1-xAlxC2 solid solutions. (c) 2007 Elsevier Ltd. All rights reserved.
关键词:
ceramics;ab initio calculations;electronic structure;electrical;conductivity;oxidation behavior;mechanical-properties;ti3sic2;temperature;ti3alc2;air;si
Philosophical Magazine
The error of Equation (15b) in my article [Z.D. Zhang, Phil. Mag. 87 (2007) p.5309] in the application of the Jordan-Wigner transformation does not affect the validity of the putative exact solution, since the solution is not derived directly from that equation. Other objections of Perk's comment [J.H.H. Perk, Phil. Mag. 89 (2009) p.761] are the same as those in Wu et al.'s comments [F.Y. Wu et al., Phil. Mag. 88 (2008) p.3093; p.3103], which do not stand on solid ground and which I have sought to refute in my previous response [Z.D. Zhang, Phil. Mag. 88 (2008) p.3097]. The conjectured solution can be utilized to understand critical phenomena in various systems, whereas the conjectures are open to rigorous proof.
关键词:
3D Ising model;exact solution;conjecture;critical phenomena;ferromagnetism;magnetic phase transition;model;analyticity