INCOMMENSURATE AND COMMENSURATE PHASE TRANSITIONS IN Ti-Ni-Fe ALLOY

RAO Jianxi Naval Academy of Engineering , Wuhan , China MA Ruzhang University of Science and Technology Beijing , Beijing , China HE Yusheng Tsinghua University , Beijing , China MA Ruzhang Professor , Department of Metal Physics , University of Science and Technology Beijing 100083 , Beijing , China

金属学报(英文版)

Measurements by using the ultrasonic technique together for electric resistance verified that the first sound velocity valley on cooling is mainly due to the soft-mode of driving the com- mensurate phase transition,and the second one due to the soft-mode of driving the martensitic transformation.The starting point,R_s,and finishing point,R_f,of the commensurate phase transition of the alloy have been determined.

关键词: incommensurate phase transition , null , null

THERMAL NUCLEATION AND GROWTH OF He BUBBLES IN He IMPLANTED STAINLESS STEELS

ZHANG Lei WANG Peixuan TAO Rong MA Ruzhang ZHANG Guoguang University of Science and Technology Beijing , Beijing , China professor , Department of Materials Physics.University of Science and Technology Beijing.Beijing 100083 , China

金属学报(英文版)

Nucleation and growth of He bubbles at different annealing temperatures T≤1023 K in stain- less steels HR-2 and SS321,implanted with He~+(40-70 keV.1×10~(16)-6× 10~(17) He~+/cm~2),were ohserved under TEM.T=0.45T_m seems to be a transition temperature.The He bubbles continue mainly their nucleation at 0.3T_m< T<0.45T_m,and grow predominantly at T≥0.45T_m,due probably to migration and coalescence by surface diffusion of metal atoms around the bubbles.The apparent activation energies for the growth are found to he 0.41 and 0.31 eV for HR-2 and SS321 respectively.The bubble density in HR-2 is greater than that in SS321 within whole measuring temperature range,and the onset temperature of rapid swelling is also higher.It is believed that the resistance of HR-2 to He is superior to that fo SS321.

关键词: stainless steel , null , null , null , null

高温退火后含He纳米晶钛膜中He相关缺陷的演化

李悦 , 邓爱红 , 刘莉 , 王康 , 谢莎

材料研究学报

利用x射线衍射(xRD)和慢正电子束分析(SPBA)技术研究高温退火后含He钛膜的微观结构和钛膜内He相关缺陷的演化.XRD分析表明,高温退火后Ti和Si在高温下发生反应形成稳定的多晶TiSi2化合物,He原子的掺入会影响TiSi2晶体的择优取向,而对TiSi2晶粒尺寸的影响较小.SPBA结果表明,室温下,钛膜内的缺陷浓度或尺寸会随着掺He浓度的增加而增大;高温退火后,当He浓度小于5%(原子分数,下同)时(除2%外),钛膜内的He相关缺陷浓度随着He浓度增加相应地增加.当He浓度增加到14%时,高温会使较高浓度的He原子、He-空位复合体以及小He泡迁移聚集形成一些尺寸较大He泡,而较大He泡周围与He相关的小尺寸缺陷的浓度则会发生相应地减少.

关键词: 金属材料 , He钛膜 , 直流磁控溅射 , He相关缺陷 , XRD , SPBA

STATISTICAL EVALUATION OF CRITICAL INCLUSION FACTOR FOR SECONDARY RECRYSTALLIZATON IN 3%Si STEEL Lecturer,Department of Materials Engineering,Southwestern Jiaotong University,Chengdu 610031,China

LI Shuchen Southwestern Jiaotong University , Chengdu , ChinaCHEN Mengzhe KE Jun University of Science and Technology Beijing , Beijing , China

金属学报(英文版)

On the basis of statistical data of MnS in the conventional 3% Si steel sheeets after various annealing processes,the critical inclusion factor has been evaluated to be 20 mm~(-1).The inhi- bition of MnS to grain growth has been exactly described.

关键词: 3%Si steel , null , null

CORRELATION BETWEEN STRESS COMPONENTS AND STRESS CORROSION CRACKS IN BRASS Lecturer,Department of Materials Physics,University of Science and Technology Beijing,Beijing 100083,China

QIAO Lijie LIU Rui XIAO Jimei University of Science and Technology Beijing , Beijing , China

金属学报(英文版)

The effects of stress components on nucleation sites and propagation directions of stress cor- rosion cracks in brass were investigated with specimens under mode Ⅱ and mode Ⅲ loadings. The results indicated that under mode Ⅱ loading,stress corrosion cracks nucleated on the site with maximum normal stress component and propagated along the plane perpendieular to the maximum normal stress,under mode Ⅲ loading,the stress corrosion crack was not evident on the 45°plane due to the general corrosion in aqueous solution with high NH_4OH concentra- tion,while stress corroded in aqueous solution with low NH_4OH concentration, numerous cracks with spacings of 10—150μm were found on the 45°plane with maximum normal stress and no stress corrosion cracks was observed on the plane with maximum shear stress.

关键词: stress corrosion cracking , null , null , null

Introduction to atmospheric corrosion research in China

Science and Technology of Advanced Materials

In this paper, we introduce the research on atmospheric corrosion in China. We describe the climate characteristics and the classification of atmospheric corrosivity across the whole country. We also describe the rusting evolution under simulated wet/dry cyclic conditions. (C) 2007 NIMS and Elsevier Ltd. All rights reserved.

关键词: atmospheric corrosion;corrosivity;rusting evolution;weathering steels;rust;mechanism;so2;o-3;no2