Laser remelting of plasma sprayed NiCrAlY and NiCrAlY-Al2O3 coatings

Yingna WU , Gang ZHANG , Bingchun ZHANG , Zhongchao FENG , Yong LIANG , Fangjun LIU

材料科学技术(英文)

Two types of plasma sprayed coatings (NiCrAlY and NiCrAlY-Al2O3) were remelted by a 5 kW cw CO2 laser. With increasing laser power and decreasing traverse speed in the ranges of 200 similar to 700 W and 5 similar to 30 mm/s respectively, the melted track grew in width and depth. In the optimum range of laser parameters, a homogeneous remelted layer without voids, cavities, unmelted particles and microcracks was formed. On the surface of remelted layers, Al2O3 and YAlO3 were detected. As a result of isothermal oxidation tests, weight gains of laser remelted coatings were obviously lower than that only plasma sprayed, especially laser remelted NiCrAlY-Al2O3 coatings. The effects of laser remelting and incorporation of Al2O3 second phase in NiCrAlY matrix on high temperature oxidation resistance were discussed.

关键词:

提高本钢265 m2冷烧结矿及原料检验代表性的实践

李凤娟 , 吕国光

金属世界 doi:10.3969/j.issn.1000-6826.2014.04.14

通过对烧结配料所需原料及对冷烧结矿成品检验采制样方法的分析,找出影响检验结果真实性的因素,采取有效的改进措施,使本钢原料厂一次配料、本钢炼铁厂265 m2烧结二次配料及265 m2烧结系统各项稳定率有了很大的提高,烧结矿实物质量和各项技术质量指标有了很大的进步,保证了高炉的稳定顺行。
  提高本钢265 m2冷烧结矿及原料检验代表性的实践
  Practice of Improving the 265 m2 Cold Sinter and Raw Material Inspection Representative
  供稿|
  李凤娟,吕国光/
  LI Feng-juan, LV Guo-guang
  DOI:10.3969/j.issn.1000-6826.2014.04.14
  导读内容
  本钢炼铁厂265 m2烧结机生产所需要的含铁原料比较复杂,一次配料料种较多,且烧结含铁原料是由本钢原料厂二车间供料,原料质量的不稳定,会影响烧结矿质量的提高和新一号高炉的强化及高炉技术指标的改善。本钢质量管理中心驻冷烧检查站加强了对烧结配料所需原料及对冷烧结矿成品检验采制样代表性的研究,采取了一些改进措施,达到了良好的效果。含铁料成分稳定率、烧结矿各项质量和技术指标在稳步地提高。下面,对本钢质量管理中心驻冷烧检查站就提高采样及检验过程的准确性所采取的措施和办法进行说明。
  烧结矿采样是半自动采样,每两小时采样一次,作为一个批次,来代表整个2h烧结矿的成份。