Determination of Neutron Irradiation-Induced Phosphorus Segregation on Grain Boundaries in a P-doped 2.25Cr1Mo Steel

Shenhua SONG , R.G.Faulkner , P.E.J. Flewitt , Dongdong SHEN , Jing LIU , Zexi YUAN

材料科学技术(英文)

Irradiation-induced impurity segregation to grain boundaries is one of the important radiation effects on materials. For this reason, phosphorus segregation to prior austenite grain boundaries in a P-doped 2.25Cr1Mo steel subjected to neutron irradiation is examined using field emission gun scanning transmission electron microscopy (FEGSTEM) with energy dispersive X-ray microanalysis (EDX). The steel samples are irradiated around 270 and 400℃, respectively. The irradiation dose rate and dose are ~1.05×10-8 dpa/s and ~0.042 dpa respectively for 270℃ irradiation, and 1.7×10-8 dpa/s and 0.13 dpa respectively for 400℃ irradiation. The FEGSTEM results indicate that there is no apparent phosphorus segregation during 270℃ irradiation but there is some during 400℃ irradiation

关键词: Neutron irradiation , null , null , null

Intensified alkaline leaching pretreatment of refractory gold concentrates at common temperature and pressure

Transactions of Nonferrous Metals Society of China

A new process for the hydrometallurgy of refractory gold concentrates was presented. The process comprises grinding-leaching, intensified alkaline leaching (IAL), cyanidation and adsorption. In a stirring-type pulverizing-leaching tower mill, the concentrate is ground to <35. 6 μm of 95. 5 % while simultaneously leached by NaOH of 12 kg/t, then carried out intensified alkaline leaching for 48 h by NaOH of 108 kg/t in enhanced agitation tanks with the pulp concentration of 40% solids at the environmental temperature of 9. 5 &SIM; 13. 5 &DEG;C and the environmental pressure of 10(5) Pa. The oxidation rate of As is 94. 9%, and 47. 6% for S. The total consumption of NaOH is only 20% of that theoretically calculated under the conditions of full oxidation at the same oxidation rates of arsenic to arsenate and sulfur to sulfate. The gold leaching rate by NaCN in 24 h is increased from 9. 2% before pretreatment to 94. 2%. The consumption of NaCN is 7. 5 kg/t, which is one times less than that before pretreatment. The extraction cost of gold is about 422 Yuan/t.

关键词: refractory gold concentrates;grinding-leaching;intensified alkaline;leaching (IAL);pretreatment;common temperature and pressure