金属学报(英文版)
A model GM (grey model) (1,1) for forecasting the rate of copper extraction during the bioleaching of primary sulphide ore was
established on the basis of the mathematical theory and the modeling process of grey system theory. It was used for forecasting the rate of copper extraction from the primary sulfide ore during a laboratory microbial column leaching experiment. The
precision of the forecasted results were examined and modified via "posterior variance examination". The results show that the
forecasted values coincide with the experimental values. GM (1,1) model has high forecast accuracy; and it is suitable for
simulation control and prediction analysis of the original data series of the processes that have grey characteristics, such as
mining, metallurgical and mineral processing, etc. The leaching rate of such copper sulphide ore is low. The grey forecasting
result indicates that the rate of copper extraction is approximately 20% even after leaching for six months.
关键词:
primary copper sulfide ore
,
null
,
null
彭宁琦
,
唐广波
,
刘正东
,
吴秀月
金属学报
doi:10.3321/j.issn:0412-1961.2009.03.013
根据Aaronson提出的超组元模型,借助Ae3的实验数据,提出了修正的置换型元素Xi(Xi=Si,Mn,Ni,Co,Mo,Al,Cu,Cr)的Zener两参数,修正中考虑了合金元素间的交互作用.修正后的超组元模型的预测精度明显改善:Ae3计算值与实验值的标准差为10.8℃,与Thermo-Calc计算值的标准差为2.35℃;Ae1计算值与实验值的标准差为6.8℃.按照马氏体相变热力学的计算方法,采用经修正的参数计算了马氏体相变开始温度Ms,提高了Ms点的预测精度,计算值与实验值的标准差为25.3℃.
关键词:
相变
,
热力学
,
超组元模型
,
相变平衡温度
盛广
,
杨志刚
金属学报
根据Fe--C--Xi合金系的正平衡和准平衡热力学模型,推导了简便的奥氏体--铁素体相变驱动力计算解析式。根据公式, 代入合金原始成分和Ae3温度, 即可准确计算正平衡和准平衡模式下的奥氏体--铁素体相变驱动力。采用这一方法计算了Fe--C--Mn--Si--Ni--Cr--Mo--Cu八元系的正平衡和准平衡奥氏体--铁素体相变驱动力。
关键词:
正平衡
,
null
,
null
,
null
马宏
,
彭晓东
,
谢卫东
腐蚀学报(英文)
利用对掺法熔铸镁合金AJ61+xY, 研究了合金中相的组成和分布及其在3.5%NaCl溶液中的腐蚀行为. 结果表明, 添加稀土Y使AJ61镁合金的晶粒明显细化,Mg17Al12 相的数量明显减少且由连续网状变成弥散颗粒状分布,沿晶界处生成耐蚀稀土相Al2Y、Al3Y, AJ61镁合金的耐腐蚀性得到明显改善. 耐腐蚀性顺序为:AJ61+1.5%Y>AJ61+2.0%Y>AJ61+1.0%Y>AJ61+0.5%Y.
关键词:
Mg-6Al-1Sr 镁合金
,
yttrium
,
microstructure
,
corrosion resistance
马宏
,
彭晓东
,
谢卫东
腐蚀学报(英文)
利用对掺法熔铸镁合金AJ61++xY,研究了合金中相的组成和分布及其在3.5%NaCl溶液中的腐蚀行为.结果表明,添加稀土Y使AJ61镁合金的晶粒明显细化,Mg17Al12相的数量明显减少且由连续网状变成弥散颗粒状分布,沿晶界处生成耐蚀稀土相Al2Y、Al3Y,AJ61镁合金的耐腐蚀性得到明显改善.耐腐蚀性顺序为:AJ61+1.5%Y>AJ61+2.0%Y>AJ61+1.0%Y>AJ61+0.5%Y.
关键词:
Mg-6Al-1Sr镁合金
,
钇
,
显微组织
,
耐腐蚀
Yan NIU
,
Weitao WU and Chaoliu ZENG (State Key Lab. for Corrosion and Protection
,
Institute of Corrosion and Protection of Metals
,
Chinese Academy of Sciences
,
Shenyang 110015
,
China)F. Gesmundo and F. Viani (Instituto di Chimica
,
Facolta di Ingegneria
,
Un
材料科学技术(英文)
The corrosion of an Fe-based alloy containing 15 wt pct Y in H2-H2S mixtures under 10-3 Pa S2 was studied at 600~800℃ in an attempt to find materials with improved sulphidation resistance with respect to pure Fe. The presence of Y has been shown to be beneflcial, but not sufficient to the level expected. In fact, the alloy is able to form at all tested temperatures an external FeS layer, beneath which a zone containing a mixture of the two sulphides is also present. Thus,Fe can still diffuse through this region to form the outer FeS layer with non-negligible rate. The corrosion rate of Fe is considerably reduced by the Y addition. but the alloy corrodes still much more rapidly than Y. The sulphidation kinetics is generally rather irregular for both the pure metals, while the corrosion rate of the alloy decreases with time and tends to become parabolic after an initial period of 12~17 h. The sulphidation behaviour of the alloys is discussed by taking into account the presence of an intermetallic compound Fe17Y2 and the limited solubility of Y in Fe
关键词:
Transactions of Nonferrous Metals Society of China
The influence of Zr and Y on the cast microstructure of a nickel-based superalloy was investigated by optical microscopy (OM), scanning electron microscopy(SEM), electron probe micro-analysis (EPMA) and X-ray diffraction (XRD). The gamma+gamma' eutectic volume in the superalloy rises notably with the increase of Zr or Y content. Meanwhile, the morphologies of primary MC carbides change from needle and platelet-like to blocky shape with increasing Zr and Y doped. The XRD results show that the primary MC carbide lattice constant increases with Zr and Y additions, and EPMA investigation shows that the platelet-like MC carbides contain primarily Nb and C, while those carbides in blocky shape have 39.2% Zr and 39.6% Nb in average,. These influences on the cast microstructure can be attributed to the atomic size effects of Zr and Y.
关键词:
yttrium;zirconium;carbides;nickel based superalloys;microstructure;solidification;carbide morphology;mechanical-properties;boron;ni3al;yttrium;sulfur