MEDIUM-RANGE ORDER CLUSTERS IN Fe-2.0 ALLOY MELT

X.B.Qin , S.J.Cheng , X.F.Bian

金属学报(英文版)

The structure of Fe-2.0 alloy melt was investigated at 1580, 1560, 1540 and 1450℃ by using an X-ray diffractometer respectively. The results showed that with decreasing temperature, the average atoms of cluster, the coordination numbers, the correlation radius and the atom density increased, whereas the pre-peak of the structure factors curve remained almost at the same position. The appearance of the pre-peak indicated that the liquid structure and the solid structure of the Fe-2.00 alloy were correlated.

关键词: liquid structure , null , null

Superconductivity modulated by internal pressure in Ce(1-x)Gd(x)FeAsO(0.84)F(0.16) compounds

Superconductor Science & Technology

It is shown that the superconductivity in Ce(1-x)Gd(x)FeAsO(0.84)F(0.16) compounds can be modulated by internal (chemical) pressure. The internal pressure is induced by Gd substitution for Ce in CeFeAsO(0.84)F(0.16), which compresses the crystal lattice. The temperature dependences of resistivity and magnetization show that the superconducting-transition temperature T(c) is enhanced from 40 K for CeFeAsO(0.84)F(0.16) to 47.5 K for Ce(0.6)Gd(0.4)FeAsO(0.84)F(0.16). The increase and subsequent decrease of Tc upon application of external pressure, as observed previously in LaFeAsO(0.89)F(0.11), is entirely confirmed by the modulation of Tc of the Ce(1-x)Gd(x)FeAsO(0.84)F(0.16) superconductors by internal pressure.

关键词: layered quaternary compound;43 k;iron

Structural evolution of Ce(1-x)Gd(x)FeAsO(0.84)F(0.16) superconductors

Journal of Applied Physics

Structural parameters have a critical impact on superconductivity in iron-based oxypnictide superconductors. Structural evolution study was performed on Ce(1-x)Gd(x)FeAsO(0.84)F(0.16) superconductors by the analysis of the x-ray diffraction patterns with Rietveld refinement. Substitution of Gd for Ce generates internal pressure that compresses the crystal lattice. The contraction of the c axis is also indicated by the reduction of Ce/Gd-As and Ce/Gd-O/F distances, while there is a slight increase in the As-Fe-As block size, which is compensated by a large reduction in the Ce/Gd-O/F-Ce/Gd block with Gd substitution. The diagonal Fe-As-Fe angle for Ce(0.6)Gd(0.4)FeAsO(0.84)F(0.16), with the highest T(c) among Ce(1-x)Gd(x)FeAsO(0.84)F(0.16) compounds, is 111.13 degrees. It is close to the ideal value of 109.47 degrees for the perfect FeAs tetrahedron, which is situated in the region of Fe-As-Fe bond angles where RFeAsO compounds tend to have the highest T(c). (C) 2011 American Institute of Physics. [doi:10.1063/1.3565408]

关键词: layered quaternary compound;high-temperature superconductivity

GdFeAsO_(1-x)F_x超导体的制备及其超导电性

崔雅静 , 陈永亮 , 杨烨 , 王雅真 , 张勇 , 赵勇

低温物理学报

通过先制备一种纳米尺寸的GdF_3作为GdFeAsO_(1-x)F_x样品中F的反应原料,在相对较低的温度(1120℃)下成功制备出一系列GdFeAsO_(1-x)F_x(x=0,0.05,0.1,0.15,0.2,0.25)多晶样品.X射线衍射结果表明,超导样品属四方ZrCuSiAs-type结构,晶格参数随着掺F量的增加而减小.扫描电子显微镜测试结果表明,样品具有片层状晶体形貌特征.当掺Fx=0.1时,样品表现出超导电性,超导转变温度为22K,随着掺F量的增多,超导转变温度升高.和其他制备方法相比,这种制备方法更有利于F的掺入,而且可有效减少样品中杂质相的含量.

关键词: 铁基超导体 , ZrCuSiAs结构

Investigations of EPR g Factors and Rhombic Distortion for the Rhombic Cu2+ Centers in K2Zn1-x Cu (x) F-4 Crystals at Low Temperature

Applied Magnetic Resonance

The electron paramagnetic resonance g factors g (i) (i = x, y, z) of two rhombic Cu2+ centers, Cu2+(II) and Cu2+(III), in K2Zn1-x Cu (x) F-4 crystals found at low temperature are calculated from the complete diagonalization (of energy matrix) method based on the cluster approach. The calculations show that the ground state wave function of the two rhombically compressed Cu2+ centers is with a small admixture of . The rhombic distortions for both Cu2+ centers are obtained from the calculations. The results are discussed.

关键词: electron-paramagnetic-resonance;atomic screening constants;hyperfine;parameters;gyromagnetic factor;spin resonance;scf functions;field;copper(ii);dependence;spectra

适用钛不同焦距X射线照相用的KUP-T-F曝光曲线

魏惠元

稀有金属材料与工程

介绍了可适用钛金属0.4 m~1.2 m不同焦距、微粒胶片X射线照相用的KUPTF新型曝光曲线的制作原理及方法.试验结果表明,新型曝光曲线具有制作简便、经济实用、可兼顾底片象质和拍片效率的优点,是钛制压力容器现场变焦距透照选取准确管电压值的理想工具.

关键词: , X射线照相 , KUPTF , 曝光曲线

用于X射线成像板的Ba7F12Cl2:Eu2+水热合成及其表征

梁庆华 , 史瑶 , 马望京 , 杨新民 , 李智

影像科学与光化学 doi:10.7517/j.issn.1674-0475.2014.02.150

X射线成像板的成像性能很大程度上取决于存储荧光粉材料的物理化学性能.本文采用水热制备方法,以BaCl2、EuBr2、NaBF4为反应原料,以乙二胺四乙酸(EDTA)为辅助剂制备了Ba7 F12 Cl2:Eu2+荧光粉.利用X射线粉末衍射(XRD)、场发射扫描电镜(SEM)、X射线能量损失谱(EDS)、拉曼光谱(Raman)、荧光光谱(PL)等对制备的Ba7 F12 Cl2:Eu2+进行了表征.根据反应条件对产物的影响,初步提出了产物的形成过程.结果表明:反应温度及EDTA用量对产物物相和形貌有显著影响;制备的Ba7 F12 C12:Eu2+荧光粉有较好的发光性能.

关键词: 荧光粉 , 水热合成 , Ba7F12Cl2 , 成像板

Theoretical studies of g factors and defect structures for cubic, tetragonal, and orthorhombic Fe+ Centers in alkali halides MX (M = Li, Na; X = F, Cl)

Communications in Theoretical Physics

The EPR g factors for cubic, tetragonal and orthorhombic Fe+ centers in alkali halides MX (M = Li, Na; X = F, Cl) are calculated from second-order perturbation formulas of g factors based on cluster approach for 3d(7) ions in three symmetries. From calculations, the g factors of these Fe+ centers in MX crystals are reasonably explained and the defect structural data for the tetragonal and orthorhombic Fe+ centers are estimated. The results are discussed.

关键词: crystal;and ligand-field theory;electron paramagnetic resonance;defect structure;atomic screening constants;spin-orbit interaction;superposition model;resonance-spectra;epr parameters;crystal-field;scf functions;ions;co2+

基于临界区加速冷却的(B+F)X80大变形管线钢的组织和性能研究

马晶 , 张骁勇 , 程时遐 , 高惠临

材料导报

采用热模拟、力学性能测试和材料显微分析等试验技术,对X80管线钢在临界区加速冷却工艺下的组织性能变化规律进行了研究.结果表明,通过临界区加速冷却,X80管线钢可获得贝氏体+铁素体(B+F)双相组织.随着始冷温度的上升,试验钢的贝氏体含量增加,铁索体含量降低,导致屈服强度增高,塑性降低.当始冷温度为840℃时,显微组织以细小、多位向分布的贝氏体为主,辅以高密度位错的多边形铁素体.这种(B+F)双相组织使得试验钢的屈强比为0.80、均匀伸长率为10.0%、形变强化指数为0.12,满足了大变形管线钢的技术要求.

关键词: X80大变形管线钢 , 临界区加速冷却 , 始冷温度

Mg-14Li-1Al-0.1Ce合金在卤素溶液(NaX,X=F, Cl, Br和I)中腐蚀行为的研究

马毅斌 , 李宁 , 黎德育 , 张密林 , 黄晓梅

腐蚀学报(英文)

用电化学方法研究了Mg-14Li-1Al-0.1Ce合金在卤素溶液(NaX, X=F, Cl,Br和I)中的腐蚀行为并用失重法测定其腐蚀速率, 用扫描电镜(SEM)观察腐蚀后的表面形貌, 利用XRD检定腐蚀产物的相组成.结果表明, 合金在卤素溶液中的腐蚀速率由低到高的顺序是:NaF<NaI<NaBr<NaCl. 经过48 h腐蚀后, 合金在NaCl、NaBr和NaI溶液中的腐蚀产物层的组分为Mg(OH)2,Li3Mg7和Li0.92Mg4.08,而在NaF溶液中的腐蚀产物层的组分为Li3Mg7和Li0.92Mg4.08. 此外, 合金在NaF溶液中的电化学活性非常低, 出现了钝化现象.电化学阻抗谱表明合金腐蚀产物层不能起到防止基体腐蚀的作用.

关键词: 镁锂合金 , corrosion , sodium halide , EIS , XRD