Distribution of Microelements and Their Influence on the Corrosion Behavior of Aluminum Foil

Weimin MAO , Heng JIANG , Ping YANG , Huiping FENG , Yongning YU

材料科学技术(英文)

The distribution of microelement Fe, Si, Cu and Mg in the surface layer of aluminum foil annealed at 300℃ and 500℃ were determined by secondary ion mass spectrometer. The corrosion structure produced by electrochemical etching was also observed. It was found that the Mg concentration at external surface was increased exponentially over the fourth degree and promoted by higher annealing temperature, which will increase the number of corrosion pits inside the large grains, and therefore the specific capacity of the foils for electrolytic capacitors. The similar effects of microelement Fe, Si and Cu were not so strong.

关键词: Electrolytic capacitor , null , null , null

Measurement and Simulation of Grain Size in Strong Textured and Coarse-Grained Metal Sheets

Leng CHEN , Weimin MAO , Yongning YU , Huiping FENG

材料科学技术(英文)

An X-ray diffractometer that equipped with a two-dimensional detector is used for developing the technique of grain size measurement for strong textured and coarse-grained Si steel sheet. The method is based on the concept that the position of diffraction spots depends on the orientation of individual grains. The two-dimensional detector has the ability to collect abundant diffraction information in seconds, thus it can be determined rapidly and accurately whether a series of diffraction spots come from the same grain. The experimental results show that this method can be used for measuring grain size and its distribution in strong textured and coarse-grained metal sheets.

关键词: Grain size , null , null

提高本钢265 m2冷烧结矿及原料检验代表性的实践

李凤娟 , 吕国光

金属世界 doi:10.3969/j.issn.1000-6826.2014.04.14

通过对烧结配料所需原料及对冷烧结矿成品检验采制样方法的分析,找出影响检验结果真实性的因素,采取有效的改进措施,使本钢原料厂一次配料、本钢炼铁厂265 m2烧结二次配料及265 m2烧结系统各项稳定率有了很大的提高,烧结矿实物质量和各项技术质量指标有了很大的进步,保证了高炉的稳定顺行。
  提高本钢265 m2冷烧结矿及原料检验代表性的实践
  Practice of Improving the 265 m2 Cold Sinter and Raw Material Inspection Representative
  供稿|
  李凤娟,吕国光/
  LI Feng-juan, LV Guo-guang
  DOI:10.3969/j.issn.1000-6826.2014.04.14
  导读内容
  本钢炼铁厂265 m2烧结机生产所需要的含铁原料比较复杂,一次配料料种较多,且烧结含铁原料是由本钢原料厂二车间供料,原料质量的不稳定,会影响烧结矿质量的提高和新一号高炉的强化及高炉技术指标的改善。本钢质量管理中心驻冷烧检查站加强了对烧结配料所需原料及对冷烧结矿成品检验采制样代表性的研究,采取了一些改进措施,达到了良好的效果。含铁料成分稳定率、烧结矿各项质量和技术指标在稳步地提高。下面,对本钢质量管理中心驻冷烧检查站就提高采样及检验过程的准确性所采取的措施和办法进行说明。
  烧结矿采样是半自动采样,每两小时采样一次,作为一个批次,来代表整个2h烧结矿的成份。