THE α_2/γ INTERFACIAL STRUCTURE CHANGES IN A DUAL-PHASE γ-TiAl ALLOY AFTER HOT DEFORMATION AND SUBSEQUENT SHORT-TIME ANNEALING

L.C. Zhang , G.L. Chen , J. G. Wang and H.Q. Ye(State Key Laboratory for Advanced Metals and Materials , University of Science and Technology Beijing , Beijing 100083 , China.)(Laboratory of Atomic Imaging of Solids , Institute of Metal Research , Chinese Academy of Sciences , Shenyang 110015 , China)

金属学报(英文版)

The nonequilibrium α2/γ interfacial structures have been studied using the conventional and high-resolution transmission electron microscope. The nonequilibrium γ/γ and α2/γ interfaces are important microstructure features of hot-forged Ti-45Al-8Nb2.5Mn-0.05B alloys. The characteristics of these nonequilibrium interfacial boundaries include the frequent interfacial ledges and the deviation from the conventional orientation relationship {111}γ.

关键词: α_2/γinterface , null , null , null

氯化钾镀锌二问问一——为何镀液中氯化钾达近400g/L?

袁诗璞

电镀与涂饰

氯化钾镀锌液配方中,氯化钾的含量通常是200~ 250 g/L,但在生产维护时分析镀槽中的氯化钾有时高达近400 g/L.认为以EDTA滴定法及硝酸银滴定法分别测总锌与总氯,然后从总氯中减去氯化锌所占氯的量而计算出氯化锌含量的常规化验方法有一定的局限性,尤其不适用于大生产已久的镀液.介绍了控制氯化钾含量的方法:先调整pH,接着通过赫尔槽试验分析并调整锌离子浓度,然后分析并调整光亮剂及硼酸,最后通过试验确定氯化钾补加量.

关键词: 镀锌 , 氯化钾 , 分析 , 调整 , 赫尔槽试验

Chen系统的状态变量周期性反馈控制

李开明 , 李亚洲 , 冯维贵 , 林长

量子电子学报 doi:10.3969/j.issn.1007-5461.2007.05.014

采用非线性反馈控制,用附加了带参数的正弦项对Chen系统进行了有效的控制.随着参数k的逐渐增大,系统的动力学行为呈现出一系列的变化.数值研究结果表明:随控制参数的增大,驱动信号的强度渐大,混沌系统由混沌运动到周期轨道,最终到一相点.

关键词: 混沌 , Chen系统 , 不动点 , Lyapunov指数 , 反馈控制

钼酸盐系列缓蚀剂在含5g/L Cl-溶液中对Q235钢的缓蚀研究

沈素峰

腐蚀学报(英文)

  通过电化学阻抗谱(EIS),研究了钼酸盐系缓蚀剂在含g">5g/L Cl-溶液中对Q235钢的缓蚀性能,结果表明:由钼酸盐为主盐与硅酸盐、磷酸盐、有机胺A复配而成的缓蚀剂,可以达到低成本、高缓蚀率的效果.并通过失重法实验对此配方进行了验证,复配缓蚀剂的缓蚀率接近88.4%,明显高于单组分缓蚀剂.

关键词: 钼酸盐 , inhibitor , compound inhibitors

钼酸盐系列缓蚀剂在含5g/L Cl-溶液中对Q235钢的缓蚀作用

沈素峰

腐蚀学报(英文) doi:10.3969/j.issn.1002-6495.2009.02.034

通过电化学阻抗谱(EIS),研究了钼酸盐系缓蚀剂在含5g/L Cl-溶液中对Q235钢的缓蚀性能,结果表明:由钼酸盐为主盐与硅酸盐、磷酸盐、有机胺A复配而成的缓蚀剂,可以达到低成本、高缓蚀率的效果.并通过失重法实验对此配方进行了验证,复配缓蚀剂的缓蚀率接近88.4%,明显高于单组分缓蚀剂.

关键词: 钼酸盐 , 缓蚀 , 复配缓蚀刺

Ion sputter erosion in metallic glass-A response to "Comment on: Homogeneity of Zr(64.13)Cu(15.75)Ni(10.12)Al(10) bulk metallic glass" by L-Y. Chen, Y-W. Zeng, Q-P. Cao, B-J. Park, Y-M. Chen, K. Hono, U. Vainio, Z-L. Zhang, U. Kaiser, X-D. Wang, and J-Z Jiang J. Mater. Res. 24, 3116 (2009)

Journal of Materials Research

The morphology of the dark and bright regions observed by transmission electron microscopy for the Zr(64.13)Cu(15.75)Ni(10.12)Al(10) bulk metallic glass strongly depends on the ion beam parameters used for ion milling. This indicates that the ion beam could introduce surface fluctuation to metallic glasses during ion milling.

关键词: room-temperature

使用安捷伦J&W DB-35ms超高惰性色谱柱和DB-XLB色谱柱对水中低于μg·L-1级的有机氯农药和除草剂进行GC/μECD法分析

Doris Smith , Ken Lynam

环境化学

本文中使用安捷伦SPEC C18AR固相萃取膜盘成功萃取了水中的有机氯农药残留和除草剂.使用双柱配置的GC/μECD系统进行检测,安捷伦J&W DB-35ms UI超高惰性色谱柱作为分析柱,DB-XLB色谱柱为确认柱.该方法为浓度接近或低于最大污染限值的含氯有机物提供了高度灵敏的分析方法.根据预估的分析物萃取浓度,方法使用的校准范围为1-100 ng· mL-1.分别对0.01 μg·L-1的加标水样和一个自来水水样进行了萃取和分析,结果证明可满足水中的有机氯农药残留和除草剂的测定.

关键词: 有机氯农药 , 除草剂 , 色谱柱

G105钻杆材料多元腐蚀行为研究

黄本生 , 江仲英 , 刘阁 , 廖周文 , 刘清友

功能材料

通过正交表设计实验,利用高温高压釜腐蚀实验并辅以失重法,研究了温度、Cl-浓度、S2-浓度和HCO3-浓度对G105钻杆材料多元腐蚀行为的影响。采用体视显微镜和SEM观察腐蚀形态和产物膜形貌,同时利用X射线能谱分析仪(EDS)进行产物膜成分分析。结果表明,在实验研究范围内,NaHCO3浓度是最大的影响因素,其次是温度和Na2S浓度,NaCl浓度的影响最小;腐蚀环境严重影响腐蚀速率;在60℃,NaCl浓度为5g/L,Na2S浓度为7g/L以及NaHCO3浓度为1g/L环境下,G105钻杆材料的腐蚀以NaHCO3引起的腐蚀为主;在60℃,NaCl浓度为50g/L,Na2S浓度为30g/L以及NaHCO3浓度为30g/L环境下,G105钻杆材料的腐蚀以Na2S引起的腐蚀为主。

关键词: G105钻杆 , 正交实验 , 高温高压腐蚀 , 多元腐蚀

用乳状液膜法分离浓缩L-苯丙氨酸

吴山 , 严忠 , 吴子生

膜科学与技术 doi:10.3969/j.issn.1007-8924.2000.03.005

以煤油-N205-P204-HCl组成的乳状液膜体系,在喷射提取柱内分别对L-苯丙氨酸及L-苯丙氨酸和L-天冬氨酸的混合溶液进行提取.实验结果表明,用1?000 mL乳状液对初始浓度为21.25 g/L的单一L-苯丙氨酸水溶液提取3次后,外相浓度降到0.95 g/L,内相最高浓度为126.10 g/L;对L-苯丙氨酸浓度为8.64 g/L的混合溶液提取两次后,外相L-苯丙氨酸浓度降至0.90 g/L,内相L-苯丙氨酸最高浓度为60.00 g/L;L-天冬氨酸的存在不影响L-苯丙氨酸的分离提取效率;每次操作溶胀均不超过26%,同时对喷射提取柱能有效减小溶胀发生的机理进行了讨论.

关键词: 乳状液膜 , L-苯丙氨酸 , L-天冬氨酸 , 分离 , 溶胀