以低压铸造用升液管为研究目的,磨切单晶硅废料Si粉和SiC为原料,Y2O3-Al2O3-Fe2O3为复合烧结助剂,反应烧结法制备Si3N4/SiC复相陶瓷.研究了Y2O3含量对复合材料结构和力学性能的影响,采用XRD、SEM对复合材料的相组成、微观形貌进行分析.结果表明,反应烧结后试样生成Si3N4结合SiC晶粒为主相的烧结体,并含有少量Sialon晶须及未反应的Si.Y2O3含量对复相陶瓷力学性能影响很大,在分析稀土Y2O3作用机理的基础上,得到2.5wt% Y2O3优化试样的力学性能优良,相对密度达到88%,维氏硬度达到1.1 GPa,常温抗弯强度50 MPa.

参考文献

[1] Koji Takahashi;Hisashi Murase;Shoko Yoshida .Improvement of static fatigue strength of Si_3N_4/SiC crack-healed under cyclic stress[J].Journal of the European Ceramic Society,2005(11):1953-1959.
[2] Luo Fa;Zhu Dongmei;Zhang Hua;Zhou Wancheng .Properties of reaction-bonded SiC/Si_3N_4 ceramics[J].Materials Science & Engineering, A. Structural Materials: Properties, Misrostructure and Processing,2006(1/2):285-289.
[3] Luo fa;Zhu dongmei;Su xiaolei;Zhou wancheng .Properties of hot-pressed of SiC/Si_3N_4 nanocomposites[J].Materials Science & Engineering, A. Structural Materials: Properties, Misrostructure and Processing,2007(1/2):7-10.
[4] S.A. Baldacim;C. Santos;O.M.M. Silva;C.R.M. Silva .Ceramics composites Si_3N_4-SiC_((w)) containing rare earth concentrate (CRE) as sintering aids[J].Materials Science & Engineering, A. Structural Materials: Properties, Misrostructure and Processing,2004(1/2):312-316.
[5] T. Hirano;K. Niihara .Microstructure and mechanical properties of Si_3N_4/SiC composites[J].Materials Letters,1995(5/6):249-254.
[6] S.A. Baldacim;C. Santos;K. Strecker .Development and characterization by HRTEM of hot-pressed Si_3N_4-SiC_(W) composites[J].Journal of Materials Processing Technology,2005(3):445-451.
[7] 岳昌盛,彭犇,郭敏,张梅.β-SiAlON晶须的诱导合成和生长机制研究[J].人工晶体学报,2011(05):1181-1187.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%