大块非晶合金具有高强度(~2 GPa),大的弹性极限(2%~3%)及良好的耐腐蚀性等优异性能,但室温塑性低限制了大块非晶合金在工程上的实际应用.本文从大块非晶合金变形与断裂的微观机制出发探讨了其室温脆性的本质,并总结了通过在大块非晶合金基体中引入第二相(外加或原位生成)来改善其室温塑性的复合韧化研究进展.
参考文献
[1] | Duwez P;Willeus R H;Klement W .[J].Applied Physics Letters,1960,31:1136. |
[2] | Zhang T et al.[J].MATERIALS TRANSACTIONS,1991,32:1005. |
[3] | Peker A;Johnson W L .[J].Applied Physics Letters,1993,63:2342. |
[4] | Lm X H;Johnson W L .[J].Journal of Applied Physics,1995,78:6514. |
[5] | Inoue A;Nishiyama N;Matsuda T .[J].Materials Transactions,1996,37:181. |
[6] | 申玉田,崔春翔,徐艳姬,韩瑞平.大块非晶合金制备原理与技术[J].稀有金属材料与工程,2004(05):459-463. |
[7] | Mark Telford .[J].Materials Today,2004,3:36. |
[8] | Kato H;Inoue A .[J].Materials Transactions,1997,38:793. |
[9] | Conner R D et al.[J].Acta Materialia,1998,46:6089. |
[10] | Szuecs F;Kim C P;Johnson W L .[J].Acta Materialia,2001,49:1507. |
[11] | Li JX.;Shan GB.;Gao KW.;Qiao LJ.;Chu WY. .In situ SEM study of formation and growth of shear bands and microcracks in bulk metallic glasses[J].Materials Science & Engineering, A. Structural Materials: Properties, Misrostructure and Processing,2003(1/2):337-343. |
[12] | Wright W J;Schwarz R B;Nix W D .[J].Materials Science and Engineering A,2001,229:319. |
[13] | Flores KM;Dauskardt RH .Enhanced toughness due to stable crack tip damage zones in bulk metallic glass[J].Scripta materialia,1999(9):937-943. |
[14] | Tan H;Zhang Y;Lia Y .[J].Intermetallics,2002,10:1203. |
[15] | Choi-Yim Haein;Conner Robert D;Szuecs Frigyes et al.[J].Scripta Materialia,2001,45:1039. |
[16] | Dragoi Danut;üstündag Ersan;Clausen Bjorn et al.[J].Scripta Materialia,2001,45:245. |
[17] | Clausen B;Lee S Y;üstündag E et al.[J].Scripta Materialia,2003,49:123. |
[18] | Choi-Yim H;Conner R D;Szuecs F et al.[J].Scripta Materialia,2001,45:1039. |
[19] | Conner R D;Dandliker R B;Johnson W L .[J].Acta Materialia,1998,46(17):6089. |
[20] | Choi-Yim H;Conner R D;Szuecs F et al.[J].Acta Materialia,2002,50:2737. |
[21] | Choi-Yim H;BuschR;Koester U et al.[J].Acta Materialia,1999,47(08):2455. |
[22] | Kim C P;Busch R;Masuhr A et al.[J].Applied Physics Letters,2001,79:1456. |
[23] | Bian Zan;Pan Mingxiang;Zhang Yun et al.[J].Applied Physics Letters,2002,81:4739. |
[24] | Hays C C;Kim C P;Johnson W L .[J].Materials Science and Engineering A,2001,650:304. |
[25] | Fan Cang;Ott R T;Hufnagel T C .[J].Applied Physics Letters,2002,81:1020. |
[26] | Inoue A .[J].Acta Materialia,2000,48:279. |
[27] | Eckert J;Küuhn U;Mattern N et al.[J].Intermetallics,2002,10:1183. |
[28] | Inoue A;Zhang T;Ishihara S et al.[J].Scripta Materialia,2001,44:1615. |
[29] | Küundig A A;Ohnuma M;Ping D H et al.[J].Acta Materialia,2004,52:2441. |
[30] | He G;Eckert J;Lüoser W .[J].Acta Materialia,2003,51:1621. |
[31] | He G;Lüoser W;Eckert J .[J].Scripta Materialia,2003,48:1531. |
[32] | Küuhn U;Eckert J;Mattern N et al.[J].Applied Physics Letters,2002,80:2478. |
[33] | Hufnagela T C;Fana Cang;Otta R T et al.[J].Intermetallics,2002,10:1163. |