研究了浓硝酸120℃回流处理不同时间后碳纳米管的形貌与结构;采用紫外分光光度计半定量表征了加入十二烷基璜酸钠后碳纳米管悬浮液浓度随时间的变化.实验发现120℃回流处理4 h可以获得长度均匀、两端开口的碳纳米管,并引入大量官能团;SDS的加入能够显著改善碳纳米管悬浮液地稳定性,加入20%SDS的悬浮液静置80 h后碳纳米管浓度仅降低10%,且沉降速度缓慢.
参考文献
[1] | Xia Z;Riester L;Curtin W A et al.[J].Acta Materialia,2004,52:931. |
[2] | Zhang Xuetong;Zhang Jin;Liu Zhongfan .[J].Carbon,2005,43:2186. |
[3] | Rong Zhong;Hongtao Cong;Pengxiang Hou .Fabrication of nano-Al based composites reinforced by single-walled carbon nanotubes[J].Carbon: An International Journal Sponsored by the American Carbon Society,2003(4):848-851. |
[4] | Jing Sun;Lian Gao;Mikio Iwasa et al.[J].Ceramics International,2005,31:1131. |
[5] | 李博,廉永福,施祖进,顾镇南.单层碳纳米管的化学修饰[J].高等学校化学学报,2000(11):1633-1635. |
[6] | 刘璐琪;郭志新;戴黎明.[J].科学通报,2001(22):151. |
[7] | Fu K;Kitaygoroskiy A;Rao AM et al.[J].NANO LETTERS,2002,2:1165. |
[8] | Kahn M G C;Banerjee S;Wong S S .[J].NANO LETTERS,2002,2:1215. |
[9] | Yang Y;Zhang J;Nan X et al.[J].Journal of Physical Chemistry B,2002,106:4139. |
[10] | Lin Y;Rao A M;Sadanadan B et al.[J].Journal of Physical Chemistry B,2002,106:1294. |
[11] | Chen X H;Chen C S;Chen Q et al.[J].Materials Letters,2002,57:734. |