用铸造及快淬工艺制备了低钴AB5型Mm(NiCoMnAl)5BxBx=0~0.2)贮氢合金,测试了合金的微观结构及电化学性能,研究了B含量及快淬工艺的变化对合金晶格常数、热力学参数、微观结构及电化学性能的影响.结果表明:合金的晶格常数、晶胞体积及标准生成焓均随B含量的增加而增大;在一定的淬速范围内,快淬处理可以提高合金的放电容量,但淬速超过某一临界淬速时,快淬合金的容量低于铸态合金;合金的循环寿命随淬速的增加而单调增加.
参考文献
[1] | Smith G;Goudy A J .[J].Journal of Alloys and Compounds,2001,316:93-98. |
[2] | Rozdzynska-Kielbik B;Iwasieczko W;Drulis H;Pavlyuk V V,Bala H .[J].Journal of Alloys and Compounds,2000,298:237-243. |
[3] | 陈立新,徐建红,雷永泉.缓冲溶液浸渍处理对贮氢合金Mm(NiCoMnAl)5电化学性能的影响[J].稀有金属材料与工程,2001(01):58-60. |
[4] | Daniel Chartouni;Felix Meli;Andreas Zuttel;Karl Gross,Louis Schlapbach .[J].Journal of Alloys and Compounds,1996,241:160-166. |
[5] | Li Chuanjian;Wang Xinlin;Wang Chongyu .[J].Journal of Power Sources,1998,74:255-260. |
[6] | 周煜;雷永泉;罗永春;王启东,成少安 .[J].金属学报,1996,32(08):857-861. |
[7] | Bowman Jr R C;Witham C;Fultz B;Ratnakumar B V,Ellis T W,Anderson I E .[J].Journal of Alloys and Compounds,1997,253-254:613-616. |
[8] | Wu Maosung;Wu Hongrong;Wang Yungyun;Wan Chichao .[J].Journal of Alloys and Compounds,2000,302:248-257. |
[9] | Mishima R;Miyamura H;Sakai T;Kuriyama N,Ishikawa H,Uehara I .[J].Journal of Alloys and Compounds,1993,192:176-178. |
[10] | Lei Y Q;Zhou Y;Luo Y C .[J].Journal of Alloys and Compounds,1997,253-254:590-593. |
[11] | Li Y;Cheng Y T .[J].Journal of Alloys and Compounds,1995,223:6-12. |
[12] | Daniel Chartouni;Felix Meli;Andreas Zuttel;Karl Gross,Louis Schlapbach .[J].Journal of Alloys and Compounds,1996,241:160-166. |
[13] | Tetsuo Sakai;Keisuke Oguro;Hiroshi Miyamura;Nobuhiro Kurayama, Akihiko Kato, Hiroshi Ishikawa .[J].Journal of the Less-Common Metals,1990,161:193-202. |