针对无机材料和复合材料的受力或变形过程中发生损伤的时间和对应载荷无法确定的难题,提出将声发射与万能材料试验机有机结合,形成一种能准确监控加载过程中损伤起始和演变的实验技术和装置.这种方法在夹层玻璃的弯曲实验和球压法测试脆性材料局部强度实验中取得了良好的效果,准确得到了发生损伤的临界载荷和反映损伤过程的载荷-声发射图.该技术对检测和预测材料的疲劳性能和失效有重要意义.

参考文献

[1] 金宗哲;包亦望.脆性材料力学性能评价与设计[M].北京:中国铁道出版社,1996
[2] 包亦望;孙立 .脆性材料在双向应力下的断裂和失效研究[J].无机材料学报,1998,13(06):847.
[3] Q.D. To;Q.-C. He;M. Cossavella .Failure analysis of tempered glass structures with pin-loaded joints[J].Engineering failure analysis,2007(5):841-850.
[4] McKenna GB .Glassy states: Concentration glasses and temperature glasses compared[J].Journal of Non-Crystalline Solids: A Journal Devoted to Oxide, Halide, Chalcogenide and Metallic Glasses, Amorphous Semiconductors, Non-Crystalline Films, Glass-Ceramics and Glassy Composites,2007(41/43):3820-3828.
[5] Chang J Y;Chou J C .Fracture strength of tempered glass[J].Journal of Non-Crystalline Solids,1982,52(1-3):395-404.
[6] Jin Z Z;Yang H .Stress-strain-acoustic emission response of glass[J].Journal of Non-Crystalline Solids,1986,80(1-3):277-282.
[7] Thomas H.Mechanical behavior of materials (英文影印版)[M].北京:机械工业出版社,2004:354-453.
[8] Y. W. Bao;S. B. Su;J. J. Yang;L. Sun;J. H. Gong .Nondestructively determining local strength and residual stress of glass by Hertzian indentation[J].Acta materialia,2002(18):4659-4666.
[9] Bao Y W;Chen J X;Wang X H et al.Shear strength and shear failure of layered machineable Ti3AlC2 ceramics[J].Journal of the European Ceramic Society,2004,24:855-860.
[10] Detian Wan;Yanchun Zhou;Chunfeng Hu .Improved strength-impairing contact damage resistance of Ti_3Si(Al)C_2/SiC composites[J].Journal of the European Ceramic Society,2007(1):2069-2076.