以诺氟沙星为水溶性模型药物,采用反相悬液冷冻凝聚法制得包裹Fe3O4微粒和药物的磁性明胶微球,考察了磁性载药微球的制备条件对微球的成球率、药物包裹率、体外释药及微球降解情况的影响.结果表明,明胶的浓度、戊二醛的用量、固化时间等均对微球的结构和性能产生影响,经优化条件得到了成球率、药物包裹率、体外释放都较好的载药微球.
参考文献
[1] | Gupta P K;Hung C T .Magnetically controlled targeted micro-carrier systems[J].Life Sciences,1989,44:175. |
[2] | Widder K J;Senyei A E;Scarpelli DG .Magnetic microspheres. A model system for the specific drug delivery in vivo[J].Society for Experimental Biology and Medicine,1978,58:141. |
[3] | Emad Eldin Hassan;Royc C Parish .Optimized Formulation of Magnetic Chitosan Microspheres Containing the Anticancer Agent, Oxantrazole[J].Pharmaceutical Research,1992,19(03):390-397. |
[4] | James M;Gallo Emad Eldin Hassan .Receptor-Mediated Magnetic Carriers:[J].Basis for Targeting Pharmaceutical Research,1988,5(05):300-304. |
[5] | 丁明;曾恒兴 .中和沉淀法Fe3O4的生成研究[J].无机材料学报,1998,13(04):619-623. |
[6] | Ida Genta;Monica Costantini;Annalia Asti et al.Influence of glutaraldehyde on drug release and mucoadhesive properties of chitosan microspheres[J].Carbohydrate Polymers,1998,36:81-88. |
[7] | 韦平原,曾毅,覃星柳.诺氟沙星葡萄糖注射液中诺氟沙星的含量测定[J].中国药事,2003(04):238-239. |