The spinodal decomposition can occur in Al-Li alloys containing 5.8-14.2 at.% Li at room temperature. The modutated structure wavelength is approximately 3.1 nm for com mercial Al-LI alloys. The limit composition of the miscibility gap is 3.66 -16.06 at.%Li at 298 K. The highest temperature of the miscibility gap is 377 K.