M-s-T curves and hysteresis loops were investigated for amorphous Fe78Si9B13, (FeNi)(78)(CrSiB)(22), their lap-wound-cores, and their composite ribbons made by two-chamber-crucible technique. The properties of the lap-wound cores of the two kinds of ribbons are similar. For the composite ribbons. the intrinsic properties are the average of the two alloys. Their technological properties, i.e., hysteresis loops, however, are no longer the average of the two alloys. Instead, they show some dramatic changes compared to the lap-wound-cores. Especially, the shape of the hysteresis loop of the composite ribbon cores is largely different from that of lap-wound-cores. The reason for the difference is supposed to be internal stress induced from cooling after annealing.