分析并优选出了甲酚甲醛树脂层压板压制过程中的温度、时间、压力及树脂成型时间4个主要工艺参数,有效解决了层压板的翘曲、开裂、厚度偏差大的问题。
Four main technical parameters including temperature, time, pressure and molding time of resin were analyzed and selected out in the pressing process of cresol formaldehyde resin laminate, and some problems such as warping, cracking and thickness deviation of the laminate were solved effectively.
参考文献
[1] | 唐传林;季承钧;单书发.绝缘材料工艺原理[M].北京:机械工业出版社,1993 |
[2] | 黄发荣;焦扬声.酚醛树脂及其应用[M].北京:化学工业出版社,2011 |
[3] | 沈仲英.酚醛及其改性树脂的示差热分析[J].浙江化工,1980(03):41-42. |