6.5%Si电工钢是一种优异的软磁材料,织构对其磁性能影响很大。利用温轧工艺对6.5%Si电工钢热轧板进行不同压下率轧制,研究了温轧板织构随压下率的变化规律。实验结果显示,随着压下率的增大,{100}〈110〉、{110}〈100〉和γ纤维织构在薄板表层中的强度先增强后减弱,当压下率达到75%时,沿板厚方向形成3个组织区域:表层细晶粒区({110}〈100〉取向为主)、过渡层({111}〈110〉和{111}〈112〉变形晶粒区)和中心层(以拉长的γ纤维织构和{100}〈110〉取向晶粒为主),这种组织和织构不均性对后期织构的发展有重大影响。

6.5wt% Si electric steel has excellent soft magnetic properties,on which texture play important role.In this experiment,warm rolling technique was employed to investigate the effect of rolling reduction on texture.It was found that the density of {100}〈110〉,{110}〈100〉 and γ-fiber textures first increased and then decreased with increasing of the rolling reduction.At 75% reduction,the microstructure along the thickness of the sheet formed three zones,containing surface layer with {110}〈100〉 orientation of refined grains,transition layer with {111}〈110〉 and {111}〈112〉 deformed grains,and center layer with elongated γ-fiber and {100}〈110〉 grains.This inhomogeneity on microstructure and texture affected the development of final texture significantly.

参考文献

[1] 何忠志.电工钢[M].北京:冶金工业出版社,1997:11-212.
[2] Haiji H;Okada K;Hiratani T et al.Magnetic proper-ties and workability of 6,5% Si steel sheet[J].Journal of Magnetism and Magnetic Materials,1996,160:109-114.
[3] Phway T P P;Moses A J .Magnetostriction trend of non oriented 6,5 Si-Fe[J].Journal of Magnetism and Mag-netic Materials,2008,320:611-613.
[4] Yong Feng Liang;F. Ye;J.P. Lin .Effect of annealing temperature on magnetic properties of cold rolled high silicon steel thin sheet[J].Journal of Alloys and Compounds: An Interdisciplinary Journal of Materials Science and Solid-state Chemistry and Physics,2010(1/2):268-270.
[5] Honma H;Ushigami Y;Suga Y .Magnetic properties of(ll0)[001-]grain oriented 6,5% silicon steel[J].Journal of Applied Physics,1991,70(10):6259-6261.
[6] 柳金龙,沙玉辉,张芳,姚勇创,李继超,左良.高硅钢薄板退火过程中的织构演变[J].功能材料,2011(11):2089-2091.
[7] Fang X S;Liang Y F;Ye F et al.Cold rolled Fe-6,5wt% Si alloy foils with high magnetic induction[J].Journal of Applied Physics,2012,111:094913.
[8] Pan Limei;Jin Jinan;Lin Junpin et al.Experimental study on the influence of boron on mechanical properties of the Fe-6,5wt% Si alloy[J].Journal of Functional Ma-terials,2003,35(06):683-685.
[9] Feng Ye;Y.F. Liang;Y.L. Wang .Fe-6.5wt.%Si High Silicon Steel Sheets Produced by Cold Rolling[J].Materials Science Forum,2010(Pt.2):1428-1433.
[10] LIANG YongFeng,YE Feng,LIN JunPin,WANG YanLi,ZHANG LaiQi,CHEN GuoLiang.Effect of heat treatment on mechanical properties of heavily cold-rolled Fe-6.5wt%Si alloy sheet[J].中国科学:技术科学(英文版),2010(04):1008-1011.
[11] Zuo Liang;Hu Guangyong;Sha Yuhui .Texture evolu-tions in Fe-6,5 //0 Si produced by rapid solidification and chemical vapor deposition[J].Journal of Materials Sci-ence Technology,2002,18(06):516-518.
[12] Barros J;Ros Yanez T;Fisher O et al.Texture devel-opment during the production of high Si steel by hot dip-ping and diffusion annealing[J].Journal of Magnetism and Magnetic Materials,2006,304:e614-e616.
[13] Zhang Z W;Chen G;Bei H et al.Improvement of magnetic properties of an Fe-6.5 % Si alloy by direction- al recrystallization[J].Applied Physics I etters,2008,93:191908.
[14] 钟太彬,林均品,陈国良.Fe3Si基合金的织构研究[J].功能材料,2000(04):361-362,365.
[15] 毛卫民;张新明.晶体材料织构定量分析[M].北京:冶金工业出版社,1993:4.
[16] Sakai T;Shiozaki M;Takashina K .A study on AIN in high permeability grain-oriented silicon steel[J].Jour nal of Applied Physics,1979,50(03):2368-2371.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%