在电化学脱氧提纯金属钇的过程中,利用熔融的CaCl2使其副产品CaO的活度降低,脱去的氧以CO或CO2气体的形式从石墨阳极放出,只要电解条件合适,可使脱氧极限无限降低,同时金属钙是由CaCl2电解所得,较Ca-CaCl2熔盐脱氧提纯金属钇的方法,它降低了由于金属Ca的不纯而引入的杂质污染.对于形状规则的金属钇脱氧时间为t=(d2/π2D)ln[(4co/πc)sinπx/d].脱氧后的产品有少量的碳污染,但对实验进行一定的改进后,也可得到氧含量和碳含量都低于100μg/g的金属钇.
参考文献
[1] | Shindo Y;Miyazaki H.[A].Sapporo Japan,1992 |
[2] | Barin I.Thermochemical Data of Pure Substances[M].Weinbeim:VCH,1989 |
[3] | Massalski T B.Binary Alloy Phase Diagrams[M].OH:American Society for Metals,1990 |
[4] | Carlson O N;Lichtenberg R R;Warner J C .[J].Journal of the Less-Common Metals,1974,35:275. |
[5] | Carlson O N;Schmidt F A;Peterson D T .[J].Journal of the Less-Common Metals,1966,10:1. |
[6] | Corbett J D;Smith J D;Carcia E .[J].Journal of the Less-Common Metals,1986,115:343. |
[7] | 李国云,李国栋,刘永林.用熔盐萃取法制备低氧稀土金属(Dy、Y)的研究[J].科学技术与工程,2004(02):106-107. |
[8] | Okabe T H;Deura T N;Oishi T .[J].Journal of Alloys and Compounds,1996,237:150. |
[9] | Okabe TH.;Kasai E.;Saito F.;Waseda Y.;Jacob KT.;Hirota K. .Thermodynamic properties of oxygen in RE-O (RE=Gd, Tb, Dy, Er) solid solutions[J].Journal of Alloys and Compounds: An Interdisciplinary Journal of Materials Science and Solid-state Chemistry and Physics,1998(2):184-191. |
[10] | Okabe T H;Oishi T et al.[J].Journal of Alloys and Compounds,1992,184:43. |
[11] | Okabe T H;Nakamura M;Oishi T .[J].Metallurgical and Materials Transactions B:Process Metallurgy and Materials Processing Science,1993,24B:449. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%