Powder of Ti-46at%Al alloy was synthesized through mechanical activation(MA) and then sintered and concurrently consolidated in a short sintering time of 900 s by using a spark plasma sintering(SPS) process. The XRD and SEM profiles show that the microstructures of TiAl alloys contained γ TiAl and small amount α-2 Ti3Al phase, whose amount can be controlled by the sintering temperature. The compacts retained the original fine-grained fully densified bodies by avoiding an excessively high sintering temperature. The alloys sintered at higher temperature with this process showed a coarser microstructure. So it is possible to produce dense nanostructured TiAl alloys by mechanically activated spark plasma sintering (MASPS) within a very short period of time.

参考文献

[1] P Bartolotta;J Barrett;T Kelly et al.The Use of Cast Ti-48Al-2Cr-2Nb in Jet Engines[J].Journal of the Minerals Metals & Materials Society,1997,49(05):48-50,76.
[2] F H Froes;C Suryanarayana;D Eliezer .Synthesis Properties and Applications of Titanium Alurninides[J].Journal of Materials Science,1992,27:5113-5140.
[3] Y W Kim;D M Dimiduk.Designing Gamma TiAl Alloys:Fundaments,Strategy and Production[J].Structural Intermetallics TMS Warrendale PA,1997:531-543.
[4] V M lmayev;G A Salishchev.An Approach to Ductility Improvement of TiAl and Ti3Al Titanium Aluminides Based on Microstructure Control[J].Structural Intermetallics TMS Warrendale PA,1997:505-514.
[5] T H Pfullmann;M Oehring;R Bohn et al.Mechanical Properties of Nanocrystalline Silicide Dispersion Strengthened (SDS)Intermetallic TiAl Alloys[J].Materials Science Forum,1996,757:225-227.
[6] C C Koch .The Synthesis and Structure of Nanocrystalline Materials Produced by Mechanical Attrition:A Review[J].Nanostructured Materials,1993,2:109.
[7] R W Boesel;M I Jacobson;I S Yoshioka .Spark Sintering Tames Exotic P-M Materials[J].Materials and Engineering,1969,70:32-35.
[8] M Omori .Sintering,Consolidation,Reaction and Crystal Growth by SPS[J].Materials Science and Engineering A:Structural Materials Properties Microstructure and Processing,2000,287:193.
[9] S Paris;E Gaffer;F Bernard et al.Spark Plasma Synthesis From Mechanically Activated Powders:A Versatile Route for Producing Dense Nanostructured Iiron Aluminides[J].Scripta Materialia,2004,50:692.
[10] Z A Munir;F Charlot;F Bernard et al.One-step Synthesis and Consolidation of Nanophase Materials[P].US 6200515,2001.
[11] E Gaffer;F Bernard .From Nanostructured Powders to Dense Nanostructured Materials:Mechanically Activated Powder Metallurgy[J].Journal of Metastable and Nanocrystalline Materials,2003,15:259.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%