A new method, using the fracture-surface topography analysis (FRASTA), of determining the parameters of rotation factor and CTOA is provided. The fracture surfaces are scanned by laser microscope and the height data is recorded to analyze. By comparing the crack extension, plastic rotation factor and COA obtained by the method of double clip gauge and by this new method respectively, the validity of it is verified. It is then used to determine the CTOA. The critical CTOA is well determined in this paper. Also by the new method, the variation of crack opening deformation ( COA and CFOA) through specimen thickness can be obtained which can't be obtained by the usual methods. It also can provide much information of crack extension such as direction and ratio.

参考文献

[1] M F Kanninen;C H Popelar.Advanced Fracture Mechanics[M].Oxford University Press,1985:77.
[2] D S Dawicke;M A Sutton;J C Jr Newman;C A Bigelow,F Erdogan.ASTM STP1220, Fracture Mechanics[M].Philadelphia,ASTM,1995:347.
[3] A A Volinsky;N Moody;W W Gerberich .[J].International Journal of Fracture,2003,119-120:431.
[4] A Cofigliano;G Maier;S Mariani .[J].Engineering Structures,1999,21:924.
[5] B Wang;K C Hwang .[J].Engineering Fracture Mechanics,1996,54(04):471.
[6] T Kobayashi;D A Shockey .[J].Current Advances in Materials and Processes,1991,11:28.
[7] Annual Book of ASTM Standards, Standard Test Method for Determining J-R Curves (E 1152-87)[M].Baltimore,ASTM,1993:853.
[8] J F Knott.Fundamentals of Fracture Mechanics[M].Butterworths,London,1973:157.
[9] Y N Liu;X L Song .[J].Engineering Fracture Mechanics,1995,52(06):1029.
[10] J S Zhao .Fracture Mechanics and Fracture Physics[D].Huazhong University of Science and Technology,2003.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%