球形化可以提高锂离子正极材料的压实密度、体积比容量并改善其加工性能和极片的质量.简要介绍了球形材料的特点,综述了球形LiCoO<,2>、LiNi<,х>M<,1-х>O<,2>、LiMn<,2>O<,4>、LiFeP0<,4>等的制备及其性能,展望了球形正极材料的应用前景.
参考文献
[1] | 吴宇平.锂离子电池[M].北京:化学工业出版社,2004 |
[2] | 王兆翔,陈立泉.锂离子电池正极材料研究进展[J].电源技术,2008(05):287-292. |
[3] | 应皆荣,高剑,姜长印,万春荣,何向明.控制结晶法制备球形锂离子电池正极材料的研究进展[J].无机材料学报,2006(02):291-297. |
[4] | Yang Chun-Chen .Synthesis and chalracterization of active materials of Ni(OH)《,2》 powders[J].Hydrogen Energy Progress,2002,27(02):1071. |
[5] | Ying Jierong;Jiang Changyin;Wan Chunrong .Preparation and characterization of high-density spherical Liz CoCh cathode material for lithium ion batteries[J].Journal of Power Sources,2004,129:264. |
[6] | 应皆荣,万春荣,姜长印.高密度球形LiCoO2的制备及性能研究[J].电源技术,2004(09):525-527. |
[7] | He Ping;Wang Haoran;Qi Lu et al.Synthetic optimization of spherical LiCO《,2》 and precursor via uniform-phase precipitation[J].Journal of Power Sources,2006,158(09):529. |
[8] | 何志奇,于利红,郑曦,朱文涛,陈立泉,邱新平.球形钴酸锂的乳液法合成及其结构、性能研究[J].化学学报,2005(24):2185-2188. |
[9] | 郭永全,尹鸽平,葛亮,李平,刘守兴.反应体系pH值和氨用量对氢氧化镍性能的影响[J].电源技术,2006(02):112-116. |
[10] | He Xiangrning;Li Jianjun;Cheng Hongwei .Controlled crvstallization and granulation of nano-scale β-Ni(OH)《,2》cathode materials for high power Ni-MH batteries[J].Polwer SOurces,2005,152:285. |
[11] | WANG Xiao-feng,RUAN Dian-bo,YOU Zheng.Application of spherical Ni(OH)2/CNTs composite electrode in asymmetric supercapacitor[J].中国有色金属学会会刊(英文版),2006(05):1129-1134. |
[12] | SungWoo Oh;Sang-Ho Park;Amine K et al.Synthesis and characterization of spherical morphology[Ni《,0.4》 Co《0.2》-Mn《,0.4》]《,3》 O《,4》 materials for lithium secondary batteries[J].Powder Sources,2006,160:558. |
[13] | ZHONG Sheng-wen,ZHAO Yu-juan,LIAN Fang,LI Yan,HU Yang,LI Pei-zhi,MEI Jia,LIU Qing-guo.Characteristics and electrochemical performance of cathode material Co-coated LiNiO2 for Li-ion batteries[J].中国有色金属学会会刊(英文版),2006(01):137-141. |
[14] | 汤宏伟,朱志红,常照荣.熔融盐法合成球形锂离子电池正极材料LiNi0.8Co0.2O2[J].河南师范大学学报(自然科学版),2008(04):89-92. |
[15] | 朱华丽,陈召勇,廖红卫,肖汉宁,肖劲.控制结晶法制备球形锰酸锂的研究[J].电源技术,2006(06):484-487. |
[16] | 何向明,蒲薇华,蔡砚,姜长印,万春荣,夏定国.基于控制结晶法制备的锂离子电池正极材料球形锰酸锂[J].中国有色金属学报,2005(09):1390-1395. |
[17] | He Xiangming;Li Jianjun;Cai Yan .Preparation of codoped sDherical sphinel LiMn《,2》O《,4》 cathode materials for Liion batteries[J].Journal of Power Sources,2005,150:216. |
[18] | Lee D K;Park S H;Amine K .High capacity Li[Li《,0.2》Ni《,0.2》-Mn《,0.6》]O《,2》 cathode materials via carbonate co-precipitation method[J].Journal of Power Sources,2006,162:1346. |
[19] | Myung Seung-Taek;Lee Myung-Hun;Kom Shinichi et al.Hydrothermal synthesis of layered LiN1l/3 Co1/3 Mn1/3 O2 as positive electrode material for lithium secondary battery[J].Electrochimica Acta,2005,50:4800. |
[20] | Deptula A;Olczak T;Lada W.[A].,2002:119. |
[21] | Pier Paolo Prosini;Maria Carewska;Silvera Scaccia;Pawel Wisniewski;Mauro Pasquali .Long-term cyclability of nanostructured LiFePO{sub}4[J].Electrochimica Acta,2003(28):4205-4211. |
[22] | 李冰,王殿龙.蜂窝结构球形LiFePO4/C的制备及性能[J].电池,2007(06):422-424. |
[23] | 于春洋,夏定国,赵煜娟,王忠丽.球形LiFePO4的制备及电化学性能[J].电池,2006(06):432-434. |
[24] | 严红,周建新,沈湘黔.反应沉淀-焙烧法制备球形LiFePO4颗粒及其微结构表征[J].过程工程学报,2008(05):983-987. |
[25] | 雷敏,应皆荣,姜长印,万春荣.高密度球形LiFePO4的合成及性能[J].电源技术,2006(01):11-13. |
[26] | Ying Jierong;Lei Min;Jiang Changyin .Preparation and characterization of high-density spherical lI0.97cR0.01fEpo4/C Ccathode material for lithium ion batteris[J].Journal of Power Sources,2006,158:543. |
[27] | 徐峙晖,赖琼钰,吉晓洋.微乳液法合成LiFePO4/C正极材料及其电化学性能[J].无机化学学报,2006(09):1610-1614. |
[28] | 侯春平,岳敏.液相球化法合成新型正极材料磷酸钒锂[J].物理化学学报,2007(12):1954-1957. |