采用等离子体辅助化学汽相沉积(PECVD)技术制备本征非晶硅薄膜,对p/i界面进行处理.在此基础上,制备P型微晶硅(μc-Si:H)薄膜与柔性太阳能电池.对P型硅薄膜及太阳能电池的性能进行研究.结果表明:对p/i界面采用H等离子体处理,再引入一定厚度的成核层,可以成功得到高电导率的P型微晶硅窗口层,提高柔性太阳能电池的光伏特性.其中的成核层,不仅促进微晶相P层的生长,还可以起到界面缓冲层的作用.

参考文献

[1] Jeffrey F;Vemstrom G .Effects of Boron Profiles on the Open Circuit Voltage of p-i-n and n-i-p Amorphous Sillcon Solar Cells[J].Applied Physics Letters,1986,48:1538.
[2] Arya R R;Catalano A;Oswald R S .Amorphous Silicon p-i-n solar Cells with Graded Interface[J].Applied Physics Letters,1986,49:1089.
[3] Rocheleau R;Hegedus S;Buchanan W et al.Novel Photochemical Vapor Deposition Reactor for Amorphous Silicon Solar Cell Deposition[J].Applied Physics Letters,1987,51:133.
[4] Guha S;Yang J;Nath P et al.Enhancement of Open Circuit Voltage in High Efficiency Amorphous Silicon Alloy Solar Cells[J].Applied Physics Letters,1986,49:218.
[5] Banerjce A .Study of Top Contact/p-layer Junction for the Optimization of Large-area Amorphous Silicon Multijunction Cells[J].Solar Energy Materials and Solar Cells,1995,36:295.
[6] Deng X;Jones S J;Liu T.VHF Plasma Depesition of μc-Si p-layer Materials[A].,1997:795.
[7] Tsai C C;Anderson G B;Thompson R.Growth of Amorphous,Microcrystalline,and Epitaxial Silicon in Low Temperature Plasma Deposition[A].,1990:475.
[8] Das UK.;Chaudhuri P.;Bhattacharyya TK. .ENHANCED BORON DOPING IN AMORPHOUS AND MICROCRYSTALLINE SILICON BY AR DILUTION[J].Journal of Physics, D. Applied Physics: A Europhysics Journal,1997(24):3371-3377.
[9] Lei Qing-Song,Wu Zhi-Meng,Geng Xin-Hua,Zhao Ying,Sun Jian,Xi Jian-Ping.Research on the optimum hydrogenated silicon thin films for application in solar cells[J].中国物理(英文版),2006(12):3033-3038.
[10] Lei Qing-Song,Wu Zhi-Meng,Geng Xin-Hua,Zhao Ying,Sun Jian,Xi Jian-Ping.Effect of substrate temperature on the growth and properties of boron-doped microcrystalline silicon films[J].中国物理(英文版),2006(01):213-218.
[11] Matsui T;Kondo M;Matsuda A .Doping properties of boron-doped microcrystalline silicon from B2H6 and BF3: material properties and solar cell performance[J].Journal of Non-Crystalline Solids: A Journal Devoted to Oxide, Halide, Chalcogenide and Metallic Glasses, Amorphous Semiconductors, Non-Crystalline Films, Glass-Ceramics and Glassy Composites,2004(0):646-650.
[12] Gordijn A;Rath J K;Schropp R E I .Role of Growth Temperature and the Presence of Dopants in Layer-by-layer Plasma Deposition of Thin Microcrystalline Silicon (μc-Si:H) Doped Layers[J].Journal of Applied Physics,2004,95:8290.
[13] Tsai C C;Anderson G B;Thomson R et al.Control of Silicon Network Structure in Plasma Depositico[J].Journal of Non-Crystalline Solids,1989,114:151.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%