高熔点(1638℃)既是NiAl的优点也是其研制的障碍之一.本文报导用热压反应烧结法制备单相NiAl和(NiAl+Ni3Al)两相金属间化合物及其室温微观组织结构和压缩力学性能.

A single NiAl phase and(NiAl+Ni3Al) two-phase intermetallics were successfully prepared by means of hot pressure reaction sintering method. The microstructures and compressive mechanical properties at room temperature also were preliminarily investigated.