采用二(2-乙基己基)磺化琥珀酸钠(AOT)作为表面活性剂,用Nd(NO3)3·nH2O与双氧水(H2O2)作为反应物,在水/AOT/甲苯的体系中,加热回流5~10 h,然后将所得到的产物自然冷却至室温,过滤、洗涤、干燥,制备出棒状NdOOH纳米粉.利用多种手段X-射线衍射(XRD)、透射电子显微镜(TEM)、热重TG及示差扫描(DSC)等手段对产物的物相、形貌、热学性能进行了表征和研究.结果表明:制备出的NdOOH纳米棒直径为100 nm、长度0.5 μm;产物在加热情况下脱水生成Nd2O3.
参考文献
[1] | Pol V G et al.[J].Journal of Physical Chemistry B,2002,106:9737. |
[2] | Wu G S et al.[J].Journal of the American Chemical Society,2004,126:5976. |
[3] | Fang Y P et al.[J].Advanced Functional Materials,2003,13:955. |
[4] | Tang Q et al.[J].Journal of Crystal Growth,2003,259:208. |
[5] | Wang X;Li Y D .[J].Chemistry-A European Journal,2003,9:5627. |
[6] | XuAW et al.[J].Journal of the American Chemical Society,2003,125:1494. |
[7] | Yada M;Mihara M;Mouri S et al.[J].Advanced Materials,2002,14:309. |
[8] | 杨儒,郭亮.纳米管状结构立方萤石型CeO2的合成[J].无机化学学报,2004(02):152-158. |
[9] | Kus S;Otremba M;Taniewski M .[J].FUEL,2003,82:1331. |
[10] | Bazzi R et al.[J].Luminescence:The Journal of Biological & Chemical Luminescence,2005,113:161. |
[11] | Dakhel AA .[J].Journal of Alloys and Compounds,2004,376:38. |
[12] | Therese G H A;Kamath P V .[J].CHEMISTRY OF MATERIALS,1999,11:3561. |
[13] | Xun Wang;Yadong Li .[J].Angewandte Chemie International Edition,2002,41:24. |
[14] | Xun Wang et al.[J].Advanced Materials,2003,15(17):66. |
[15] | Bazzia R et al.[J].Journal of Luminescence,2003,102-103:445. |
[16] | 黄普选,何斌,吴锋,潘桂玲,高学平.钕的氢氧化物和氧化物纳米线的制备及表征[J].无机化学学报,2006(04):639-644. |
[17] | Mahiko Nagao et al.[J].Langmur,2003,19:9201. |
[18] | Tong J;Eyring L .[J].Journal of Alloys and Compounds,1995,225:139. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%