采用溶胶-凝胶法合成了Ba0.5Sr0.5Al2Si2O8(BSAS)-Y2Si2 O7粉体,并以2D Cf/SiC为基体,采用浆料涂覆工艺在其表面制备了BSAS-Y2Si2O7环境屏障涂层,表征了涂覆与未涂覆BSAS-Y2Si2O7涂层Cf/SiC复合材料的抗水氧腐蚀性能.结果表明:在高纯氩气保护下,经1450℃高温烧结3h,可在Cf/SiC试样表面制备致密的BSAS-Y2Si2O7涂层;在1250℃、50%H2O-50%O2、常压静态气氛下腐蚀200 h后,涂覆BSAS-Y2Si2O7涂层的Cf/SiC试样的质量基本不变,基体中的纤维得到了很好的保护,所制备的BSAS-Y2Si2O7涂层具有较好的抗水氧腐蚀性能;同时,BSAS-Y2Si2O7涂层也表现出裂纹自愈合能力;与之相比,未涂覆BSAS-Y2Si2O7涂层的Cf/SiC试样的失重较为明显,基体中的纤维已经完全被水氧环境所侵蚀.
参考文献
[1] | 张立同,成来飞,徐永东.新型碳化硅陶瓷基复合材料的研究进展[J].航空制造技术,2003(01):24-32. |
[2] | Schiroky G H .Oxidation behavior of chemically vapor-deposited silicon carbide[J].ADVANCED CERAMIC MATERIALS,1987,2(02):137. |
[3] | Schmidt S;Beyer S;Knabe H et al.Advanced ceramic matrix composites materials for current and future propulsion technology applications[J].Acta Astronautica,2004,55(3-9):409. |
[4] | Jacobson N S .Corrosion of silicon-based ceramics in combustion environments[J].Journal of the American Ceramic Society,1993,76(01):3. |
[5] | Smialek JL.;Opila EJ.;Fox DS.;Jacobson NS.;Robinson RC. .SiC and Si3N4 recession due to SiO2 scale volatility under combustor conditions[J].Advanced Composite Materials: The Official Journal of the Japan Society of Composite Materials,1999(1):33-45. |
[6] | Wang Y G;Fei W F;Fan Y et al.Silicoaluminum carbonitride ceramic resistance to oxidation/corrosion in water vapor[J].Journal of Materials Research,2006,21(07):1625. |
[7] | Jacobson N S .Kinetics and mechanism of corrosion of SiC by molten salts[J].Journal of the American Ceramic Society,2005,69(01):74. |
[8] | Tressler R E et al.Molten salt corrosion of SiC and Si3N4ceramics[J].Journal of the American Ceramic Society,2006,59(5-6):278. |
[9] | Lee K N .Current status of environmental barrier coatings for Si-based ceramics[J].Surface and Coatings Technology,2000,133-134:1. |
[10] | Lee K N et al.Development and environmental durability of mullite and mullite/YSZ dual layer coatings for SiC and Si3N4 ceramics[J].Surface and Coatings Technology,1996,86-87(01):142. |
[11] | Lee KN. .Key durability issues with mullite-based environmental barrier coatings for Si-based ceramics[J].Journal of engineering for gas turbines and power: Transactions of the ASME,2000(4):632-636. |
[12] | Kang N. Lee;Dennis S. Fox;Jeffrey I. Eldridge .Upper Temperature Limit of Environmental Barrier Coatings Based on Mullite and BSAS[J].Journal of the American Ceramic Society,2003(8):1299-1306. |
[13] | Wang Y G;Liu J L .Water corrosion behaviors of barium aluminosilicates:A first-principles investigation[J].Corrosion Science,2009,51(09):2126. |
[14] | Wang Y G et al.Hot corrosion behavior of barium aluminosilicate-coated C/SiC composites at 900 ℃C[J].Journal of the American Ceramic Society,2010,93(01):204. |
[15] | Jia Liu;Litong Zhang;Qiaomu Liu .Polymer-Derived SiOC-barium-strontium aluminosilicate Coatings as an Environmental Barrier for C/SiC Composites[J].Journal of the American Ceramic Society,2010(12):4148-4152. |
[16] | Lee K N;Fox D S;Bansal N P .Rare earth silicate environmental barrier coatings for SiC/SiC composites and Si3 N4 ceramics[J].Journal of the European Ceramic Society,2005,25(10):1705. |
[17] | Hong Z L;Cheng L F;Zhang L T et al.Water vapor corrosion behavior of scandium silicates at 1400 ℃[J].Journal of the American Ceramic Society,2009,92(01):193. |
[18] | Yiguang Wang;Jinling Liu .First-principles investigation on the corrosion resistance of rare earth disilicates in water vapor[J].Journal of the European Ceramic Society,2009(11):2163-2167. |
[19] | Jia Liu;Litong Zhang;Juan Yang .Fabrication of SiCN-Sc_2Si_2O_7 coatings on C/SiC composites at low temperatures[J].Journal of the European Ceramic Society,2012(3):705-710. |
[20] | Jia Liu;Litong Zhang;Fei Hu .Polymer-derived yttrium silicate coatings on 2D C/SiC composites[J].Journal of the European Ceramic Society,2013(2):433-439. |
[21] | Zhu D M;Bansal N P;Miller R A .Thermal conductivity and stability of hafnia-and zirconate-based materials for 1650 ℃ thermal/environmental barrier coating application[J].Ceramic transactions,2003,153:331. |
[22] | 鲁琳静 .BSAS系环境障碍涂层的制备与耐水腐蚀性能研究[D].西安:西北工业大学,2011. |
[23] | Ramasamy, S.;Tewari, S.N.;Lee, K.N.;Bhatt, R.T.;Fox, D.S. .Mullite-gadolinium silicate environmental barrier coatings for melt infiltrated SiC/SiC composites[J].Surface & Coatings Technology,2011(12):3578-3581. |
[24] | 鲁琳静,成来飞,洪智亮,王一光,张立同.Ba0.25Sr0.75Al2Si2O8环境障碍涂层的制备与耐水腐蚀性能研究[J].无机材料学报,2011(07):701-706. |
[25] | 殷小玮 .3DC/SiC复合材料的环境氧化行为[D].西北工业大学,2001. |