通过熔融缩聚法制备了具有良好成膜性的聚乳酸-聚乙二醇共聚物(PLEG),并采用低能电子束辐射改性PLEG薄膜,研究了辐射剂量对其拉伸性能和断裂伸长率的影响.结果表明,当加入3%的三聚氰酸三烯丙酯(敏化剂TAC),以80 kGy的剂量辐射后,5#和6# PLEG薄膜的综合力学性能达到最佳,凝胶率分别为54.3%和73.9%,拉伸强度为12.3 MPa和20 MPa,断裂伸长率为283%和29%.
参考文献
[1] | Kulinski Z;Piorkowska E;Gadzinowska K .[J].Biomacromolecules,2006,7:2128-2135. |
[2] | Tuominen J.;Seppala JV. .Synthesis and characterization of lactic acid based poly(ester-amide)[J].Macromolecules,2000(10):3530-3535. |
[3] | Nagasawa N;Kaneda A;Kanazawa S et al.[J].Nuclear Instruments and Methods in Physics Research B:Beam Interaction with Materials and Atoms,2005,236:611-616. |
[4] | Mitomo H;Kaneda A;Quynh TM;Nagasawa N;Yoshii F .Improvement of heat stability Of poly(L-lactic acid) by radiation-induced crosslinking[J].Polymer: The International Journal for the Science and Technology of Polymers,2005(13):4695-4703. |
[5] | 张亨.三聚氰酸三烯丙酯的合成[J].塑料助剂,2003(04):16-18. |
[6] | Kai-Lai G;Pometto A L .[J].Journal of Environmental Polymer Degradation,1999,7:93-100. |
[7] | Kantoglu O.;Guven O. .Radiation induced crystallinity damage in poly(L-lactic acid)[J].Nuclear Instruments and Methods in Physics Research, Section B. Beam Interactions with Materials and Atoms,2002(3/4):259-264. |