通过传统的固相烧结法合成(1-x)(Bi0.5Na0.5)TiO3-x(Bi0.5K0.5)TiO3陶瓷(x选取范围0.135~0.24).先在850 ℃合成原料粉体,然后在1100~1200 ℃下烧结得到陶瓷样品.分析检测该体系陶瓷的结构以及铁电、压电性能.X射线衍射分析结果表明,该二元系准同型相界(MPB)区域位于x=0.165~0.225附近.对这一体系铁电和压电性能进行测试,并对其在准同型相界附近的电学性能发生变化的机理作了讨论.(Bi0.5Na0.5)TiO3-(Bi0.5K0.5)TiO3是一种很有应用前景的无铅压电陶瓷材料,值得进一步的研究和探索.同时,本实验还对密封烧结工艺对无铅压电陶瓷性能的影响作了初步的研究.
参考文献
[1] | Tadashi Takenaka;Hajime Nagata .Current status and prospects of lead-free piezoelectric ceramics[J].Journal of the European Ceramic Society,2005(12):2693-2700. |
[2] | Saito Y;Takao H;Tani T et al.[J].NATURE,2004,432(7013):84. |
[3] | Junjie Hao;Xiaohui Wang;Renzheng Chen et al.[J].Materials Chemistry and Physics,2005,90:282. |
[4] | Pusit Pookmanee;Gobwute Rujijanagul et al.[J].Journal of the European Ceramic Society,2004,24:517. |
[5] | Hong-Wei Cheng;Xue-Jin Zhang et al.[J].Applied Physics Letters,2004,85:2319. |
[6] | Yet-Ming Chiang;Gregory W et al.[J].Applied Physics Letters,1998,73:3683. |
[7] | Atsushi Sasaki;Tatsuya Chiba;Youichi Mamiya;Etsuo Otsuki .Dielectric and Piezoelectric Properties of (Bi_(0.5)Na_(0.5))TiO_3-(Bi_(0.5)K_(0.5))TiO_3 Systems[J].Japanese journal of applied physics,1999(9B):5564-5567. |
[8] | Suchuan Zhao;Guorong Li;Aili Ding et al.[J].Journal of Physics D:Applied Physics,2006,39:2277. |
[9] | WEN CHEN;YUEMING LI;QING XU;JING ZHOU .Electromechanical Properties and Morphotropic Phase Boundary of Na{sub}0.5Bi{sub}0.5TiO{sub}3-K{sub}0.5Bi{sub}0.5TiO{sub}3-BaTiO{sub}3 Lead-free Piezoelectric Ceramics[J].Journal of electroceramics,2005(3):229-235. |
[10] | Yueming Li;Wen Chen et al.[J].Materials Letters,2005,59:1361. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%