An investigation was performed on the effects of semi-solid compression parameters,such as strain rate,compression temperature and heating time at these temperatures on deformation behaviors of two kinds of ZA27 alloys,one was modified by Zr and the other was unmodified.The results indicate that with the increasing of the strain,the stress of the modified composite first sharply increases to a peak value,then dramatically decreases to a plateau value,and again increases till the end of deformation.But for the unmodified,after being up to a peak value,the stress only decreases slowly.As the compression temperature or the heating time decreases,or the strain rate increases,the stress level and the cracking degree of these two kinds of alloys increase.Under the same deformation conditions,the stress level and the cracking degree of the unmodified alloy are higher than those of the modified one.But there is an exception that the stress level of the unmodified alloy is minimum and smaller than that of the modified one when deformed at the low temperature of 450℃.These phenomena were mainly discussed through analyzing the microstructures under different conditions and the deformation mechanisms at different deformation stages.
参考文献
[1] | Prasad BK.;Patwardhan AK.;Yegneswaran AH. .INFLUENCE OF THE NATURE OF MICROCONSTITUENTS ON THE TENSILE PROPERTIES OF A ZINC-BASED ALLOY AND A LEADED-TIN BRONZE AT DIFFERENT STRAIN RATES AND TEMPERATURES[J].Journal of Materials Science,1997(5):1169-1175. |
[2] | Prasad BK.;Patwardhan AK.;Yegneswaran AH. .INFLUENCE OF THE NATURE OF MICROCONSTITUENTS ON THE TENSILE PROPERTIES OF A ZINC-BASED ALLOY AND A LEADED-TIN BRONZE AT DIFFERENT STRAIN RATES AND TEMPERATURES[J].Journal of Materials Science,1997(5):1169-1175. |
[3] | Barnhurst R J;Jacob D .Gravity Casting of Zinc-aluminum Zlloys:Development of Foundry Parameters for Casting in Sand[J].AFS Transactions,1998,96:321-328. |
[4] | 陈体军,郝远.金属的半固态成形技术与应用[J].铸造,2001(11):645-649. |
[5] | Chen C P;Tsao C-Y A .Semi-solid Deformation of Aluminum Alloy 356 with Non-dendritic Structure[J].Materials Science and Technology,1999,15:981-985. |
[6] | Chen CP.;Tsao CYA. .RESPONSE OF SPRAY-DEPOSITED, STIRRED-CAST AND CONVENTIONAL CAST PB-SN ALLOYS TO DEFORMATION IN THE SEMI-SOLID STATE[J].Journal of Materials Science,1995(16):4019-4026. |
[7] | Freitas E R;Ferrante M .Reological Behavior and Deformation Characteristics of a Commercial and a Laboratory-cast Al-4%Cu Alloy in the Semi-solid State[J].Acta Materialia,2001,49:3839-3847. |
[8] | Tzimas E.;Zavaliangos A. .Mechanical behavior of alloys with equiaxed microstructure in the semisolid state at high solid content[J].Acta materialia,1999(2):517-528. |
[9] | Chen C P;Tsao C-Y A .Semi-solid Deformation of Non-dendritic Structures-Ⅰ[J].Phenomenological Behavior Acta Mater,1997,45:1955-1968. |
[10] | CHEN Ti-jun,MA Ying,HAO Yuan,Lu Song,XU Guang-ji,SUN Jun.Structural evolution of ZA27 alloy during semi-solid isothermal heat treatment[J].中国有色金属学会会刊(英文版),2001(01):98-102. |
[11] | Chen T J;Hao Y;Sun J.Microstructural and Constitutional Evolution of Cast Dendritic ZA27 Alloy during Partial Remelting[J].J Mater Processing Technol |
[12] | Evangelos Tzimas;Antonios Zavaliangos .Evolution of near-equiaxed microstructure in the semisolid state[J].Materials Science & Engineering, A. Structural Materials: Properties, Misrostructure and Processing,2000(1/2):228-240. |
[13] | 陈体军,郝远,陆松,许广济.ZA27合金在SIMA处理过程中形变量和等温温度对组织的影响[J].金属热处理学报,2000(01):26-31. |