The aim of the work was to find out how the modification of surface treatment and microstructures affect the fatigue characteristics of the considered sintered materials. Two different systems were prepared: as-sintered and shot peened prealloyed sintered (Astaloy CrL based) steels with addition of 0.5% and 0.7% C. Sintering was carried out in laboratory tube furnace in an atmosphere of pure gases 75%N_2+25%H_2. The sintering temperature was 1180℃ and sintering time was 60 min. Heating and cooling rates were 10℃/min. Fatigue tests were carried out in symmetric plane bending at stress ratio R=-1 with frequency of about 24 Hz. The presented experimental results showed that prealloyed water-atomised steels, with surface modification, exhibit positive effects on the fatigue failure resistance, and for that reason are suitable for high-performance applications.

参考文献

[1] [J].Technical Trends:Met Powder Rep,2004,59(05):26.
[2] C.M.Sonsino .[J].Powder Metallurgy,1990,33(03):235.
[3] V. Bacova;D. Draganovskd .Analyses of the Quality of Blasted Surfaces[J].Materials Science,2004(1):125-131.
[4] M.Mihalikova;M.Bursak;J.Michel';K.Ko-valova .[J].J Met Mater Min,2005,15(02):53.
[5] D.Kniewald;J.Brezinova;A.Guzanova .[J].Communications,2004,6(02):37.
[6] F. NOVY;P. PALCEK;M. CHALUPOVA .Failure of Al-alloy AK 4-1 under creep-fatigue interaction conditions[J].Kovove materialy,2005(6):447-456.
[7] F.Novy;M.Cincala;P.Kopas;O.Bokuvka .[J].Materials Science and Engineering,2007,462A:189.
[8] G.F.Bocchini .[J].Rev Powder Metall Phys Ceram,1985,2(04):313.
[9] R.Bidusky;M.Actis-Grande .[J].High Temperature Materials and Processes,2008,27(04):249.
[10] E.Dudrova;M.Kabatova;R.Bidulsky.[A].Cluj-Napoca,TU,2005:101.
[11] V.Simkulet;M.Selecka .[J].Powder Metall Prog,2006,6(04):156.
[12] M. Kabatova;E. Dudrova;A.S. Wronski .Fracture micromechanics of static subcritical growth and coalescence of microcracks in sintered Fe-1.5Cr-0.2Mo-0.7C steel[J].Powder Metallurgy,2006(4):363-368.
[13] H. Danninger;U. Sonntag;B. Kuhnert .Automatische Messung des effektiven tragenden Querschnitts A_c in Sinterstahl[J].Practical Metallography,2002(8):414-425.
[14] G.Rosenberg .[J].Metalurgija,2001,40(01):13.
[15] J.R.Moon .[J].Powder Metall Prog,2002,2(02):63.
[16] D.Rodzinak;M.Slesar .[J].Powder Metallurgy International,1980,12(03):127.
[17] R.C O'Brien .[J].Metal Powder Report,1988,43:744.
[18] J.Bidulska;T.Kvackaj;V.Bodak .[J].Hutnicke Listy,2002,57(1-3):11.
[19] J.Bidulska;T.Kvackaj;V.Bodak;R.Rakuciak .[J].Acta Metallurgica Slovaca,2002,8:211.
[20] A.Guzanova;J.Brezinova .[J].J Met Mater Min,2008,18(02):7.
[21] S. Tekeli .Enhancement of fatigue strength of SAE 9245 steel by shot peening[J].Materials Letters,2002(3):604-608.
[22] L.Ceniga .[J].Journal of Thermal Stresses,2008,31(08):728.
[23] L.Ceniga .[J].Journal of Thermal Stresses,2008,31(09):862.
[24] Y.K.Gao;M.Yao;J.K.Li .[J].Metallurgical and Materials Transactions A:Physical Metallurgy and Materials Science,2002,33A:1775.
[25] A. C. Batista;A. M. Dias J. L. Lebrun;J. C. Le Flour;G. Inglebert .Contact fatigue of automotive gears: evolution and effects of residual stresses introduced by surface treatments[J].Fatigue & Fracture of Engineering Materials and Structures,2000(3):217-228.
[26] M. Guagliano;L. Vergani .An approach for prediction of fatigue strength of shot peened components[J].Engineering Fracture Mechanics,2004(4/6):501-512.
[27] K.Kanno;Y.Takeda;A.Bergmark;L.Alzati,B.Lindqvist,Y.Ueda,K.Kanda and A.Zandonati.[A].EPMA,Shrewsbury,2004:178.
[28] H.Karlsson;L.Nyborg;O.Bergman.[A].EPMA,Shrewsbury,2004:24.
[29] U.Engstrom;K.Lipp;C.M.Sonsino.[A].MPIF,Princeton,2001:10,1.
[30] O.Bergman;A.Bergmark.[A].MPIF,Princeton,2003:270.
[31] S.L.Sigl;P.Delarbre.[A].MPIF,Princeton,2003:54.
[32] H.Danninger;C.Gierl .[J].International Journal of Materials and Product Technology,2007,28(3-4):338.
[33] R.Bidulsky;D.Rodzinak;A.Guzanova;J.Brezinova .[J].Acta Metallurgica Slovaca,2006,12(01):54.
[34] M.Kabatova;E.Dudrova;A.S.Wronski;R.Bidulsky .[J].Powder Metall Prog,2007,7(01):20.
[35] G.Piotrowski;X.Deng;N.Chawla;K.S.Narasimhan.[A].EPMA,Shrewsbury,2004:152.
[36] P. S. Song;C. C. Wen .Crack closure and crack growth behaviour in shot peened fatigued specimen[J].Engineering Fracture Mechanics,1999(3):295-304.
[37] Y.K.Gao;X.B.Li;Q.X.Yang;M.Yao .[J].Materials Letters,2007,61(01):466.
[38] F.Novy;M.Chalupova;M.Cincala;O.Bokuvka .[J].Acta Mech Slov,2007,11(04):189.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%