在压力为3-6GPa和温度为723-933K范围内,对非晶(Fe_(0.99)Mo_(0.01))_(78)Si_9B_(13)合金等温晶化形成的纳米α-Fe(Mo,Si)晶粒尺寸随温度和压力的变化进行了研究。发现其晶粒尺寸随压力变化主要取决于压力对成核速率的影响,其根本原因是压力对熔点的作用;而压力亦影响生长速率,但对最小晶粒尺寸的形成温度和临界压力的影响可以忽略.

Effects of pressure and temperature on grain size of nanocrystalline α-Fe(Mo,Si) produced by annealing amorphous (Fe_(0.99)Mo_(0.01)_(78)Si_9B_(13) alloys in temperature range from 723 to 933 K under pressures range of 3 to 6 GPa were studied. It is found that the effect of pressure on α-Fe(Mo,Si) grain size results mainly from nucleation rate, and its basic cause is the effect on melting point. Yet the effect of pressure, decreasing growth rate, on the fomiation temperature and critical pressure of smallest grain size of α-Fe(Mo,Si) can be negligible. Correspondent: (YAO Bin, associate professor, Physics Department, Siping Normal College,Siping 136000)

参考文献

[1]
[2]
[3]
[4]
[5]
[6]
[7]
[8]
[9]
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%