欢迎登录材料期刊网

材料期刊网

高级检索

The internal friction (IF) of Mg-0.6%Zr alloy is measured in the present study and two IF peaks of (P1 (97 ℃,1 Hz) and P2 (230 ℃,1Hz)) are found,respectively.It is shown that the novel P1 peak is frequency independent and the peak tempera- ture increased with the increase of strain amplitude or heating rate.P1 peak could be repressed by the reheating-up measurements and represented by heat treatment.The mechanism of P1 peak is clarified by optical microscope (OM) and transmission electron microscope (TEM) observation,and considered to be caused by the creation and expansion of dislocations during plastic deformation.The P2 peak is a thermally activated relaxation IF peak,and activation energy is 1.46 eV,which is caused by the relaxation of the grain boundaries in Mg-0.6%Zr alloy.

参考文献

[1] X.S. Hu;Y.K. Zhang;M.Y. Zheng .A Study of Damping Capacities in Pure Mg and Mg-Ni Alloys[J].Scripta materialia,2005(11):1141-1145.
[2] I.S. Golovin .Damping Mechanisms in High Damping Materials[J].Key engineering materials,2006(319):225-230.
[3] A. MUNITZ;R.E. RICKER;D.J. PITCHURE .The Influence of Thermomechanical Treatment on the Complex Modulus of Mg Alloy AZ31[J].Metallurgical and Materials Transactions, A. Physical Metallurgy and Materials Science,2005(9):2403-2413.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%