Several gelatin-silicate composites, with or without incorporation of Ca2+ ions, were synthesized through sol-gel processing starting from gelatin and 3-(glycidoxypropyl) trimethoxysilane. The structure around the Si atoms was similar for all the samples. The measurement of viscoelastic properties indicated that the glass transition temperature and activation energy decreased with the incorporation of Ca2+ ions. The Ca2+ ion-containing composites were bioactive as they spontaneously deposited apatite when soaked in a simulated body fluid of the Kokubo recipe.
参考文献
[1] | L L Hench;J Wilson.[J].An Introduction to Bioceramics World Scientific Singapore,1993 |
[2] | J-P Draye;B Delaey;A Van De;A Van Den BulckeB Bogdanov and E Schacht .[J].Biomaterials,1998,19:99. |
[3] | M N Taravel;A Domard .[J].Biomaterials,1995,16:865. |
[4] | S M Jones;S E Friberg .[J].Journal of Materials Science,1994,29:4075. |
[5] | Yoshinaga;N Yamada;S Katayama .[J].Materials Research Society Symposium Proceedings,1998,519:285. |
[6] | K Tsuru;C Ohtsuki;A Osaka;T Iwamoto and J D Mackenzie .[J].Journal of Materials Science:Materials in Medicine,1997,8:157. |
[7] | P Müller;C Becker;S Schmidt .[J].Materials Research Society Symposium Proceedings,1998,519:389. |
[8] | R H Glaser;G L Wilkes .[J].Journal of Non-Crystalline Solids,1989,113:73. |
[9] | S B Ross-Murphy .[J].POLYMER,1992,33:2622. |
[10] | R Wüstneck;E Buder;R Wezel;H Hermel .[J].Colloid and Polymer Science,1989,267:429. |
[11] | C Ohtsuki;T Kokubo;K Takatsuka;T Yamamura .Nippon Seramikusu Kyokai Gakujutsu Ronbunshi[Z].,1991. |
[12] | M M Pereira;L L Hench .[J].Journal of Sol-Gel Science and Technology,1996,7:59. |