在理论研究和试验的基础上,结合各研究者实验数据和作者的大量研究结果,研究了奥氏体不锈钢室温强度和塑性与合金元素的变化规律,经计算机处理得到了室温强度、伸长率的定量计算的表达式.
参考文献
[1] | LI Dong-Sheng;CHEN Xi-Zhang;DAI Qi-Xun .Calculation and analysis of microstructure of austenitic steel for supercritical unit[J].Applied Mechanics and Materials,2011,84-85:337-341. |
[2] | Dai Q X;Wang A D;Cheng X N et al.Stacking fault energy of cryogenic austenite steels[J].Chinese Physics,2002,11(06):596-600. |
[3] | Dai Qixun;Cheng Xiaonong;Luo Xingming et al.Structural parameters of martensite transformation for austenitic steels[J].Materials Characterization,2003,49(04):367. |
[4] | Dai QX;Yuan ZZ;Luo XM;Cheng XN .Numerical simulation of Cr2N age-precipitation in high nitrogen stainless steels[J].Materials Science & Engineering, A. Structural Materials: Properties, Misrostructure and Processing,2004(1/2):445-448. |
[5] | 肖纪美.不锈钢的金属学问题[M].北京:冶金工业出版社,2006 |
[6] | Kamachi Mudali U;BaldeV Raj;李晶;黄运华.高氮钢和不锈钢——生产、性能与应用[M].北京:化学工业出版社,2006 |
[7] | 俞德刚.钢的强韧化理论与设计[M].上海:上海交通大学出版社,1990 |
[8] | 赵进刚,张宝伟,王明林.高强度奥氏体不锈钢的发展[J].材料开发与应用,2005(04):38-40. |
[9] | 陆世英;张廷凯;康喜范.不锈钢[M].北京:原子能出版社,1998 |
[10] | 程晓农,李丹,戴起勋,李冬升,吴青松,王志健.超临界锅炉用不锈钢热处理工艺与组织分析[J].江苏大学学报(自然科学版),2009(05):475-478. |
[11] | 程晓农;戴起勋.奥氏体钢设计与控制[M].北京:国防工业出版社,2005 |
[12] | Peckner D;Bernsterain I M;顾守仁.不锈钢手册[M].北京:机械工业出版社,1987 |
[13] | Tobler R L;Meyn D .Cleavage-like fracture along slip planes in Fe-18Cr-3Ni-13Mn-0 37N austenitic stainless steel at liquid helium temperature[J].Metallurgical and Materials Transactions A:Physical Metallurgy and Materials Science,1988,19:1626-1631. |
[14] | Reed R P;Tobler R L;Elmer J M.Strength and toughness of USSR Fe-20Cr-16Ni-6Mn-0,2N weldments at cryogenic temperature[A].Geneva.IPC Science and Technology Press,1980:797-801. |
[15] | 张彦生;师昌绪 .铁-锰-铝系奥氏体钢--耐热钢、无磁钢和低温钢[J].金属学报,1964,7(03):285-300. |
[16] | 孙玉梅,邹小平.Super304H不锈钢锅炉管评述[J].锅炉技术,2007(01):52-55. |
[17] | 周勇,郎宇平,荣凡,刘培英.奥氏体不锈钢15Mn-22Cr-0.56N的热塑性和轧制工艺对其性能的影响[J].特殊钢,2008(01):22-24. |
[18] | Jiao F.;Portella PD.;Ziebs J.;Osterle W. .BIAXIAL PATH-DEPENDENCE OF LOW-CYCLE FATIGUE BEHAVIOUR AND MICROSTRUCTURE OF ALLOY 800 H AT ROOM TEMPERATURE[J].Materials Science & Engineering, A. Structural Materials: Properties, Misrostructure and Processing,1995(1/2):19-24. |
[19] | R. Dehmolaei;M. Shamaman;A. Kermanpur .Microstructural changes and mechanical properties of Incoloy 800 after 15 years service[J].Materials Characterization,2009(3):246-250. |
[20] | 马玉喜,荣凡,周荣,郎宇平,蒋业华.超高氮奥氏体钢的韧-脆转变[J].钢铁,2008(02):89-92,100. |
[21] | 胡本芙,鹿林,贾成厂,木下博嗣,高桥平七郎.(C+N)复合强化的Fe-Cr-Mn(W,V)钢高温性能的研究[J].钢铁,2000(03):46-51. |
[22] | 赵朴.化学成分和固溶温度对1Cr17Mn9Ni4N不锈钢组织和性能的影响[J].钢铁研究学报,2003(03):21-24. |
[23] | 《手册》编委会.火力电厂金属材料手册[M].北京:中国电力出版社,2001 |
[24] | 徐祖耀 .Fe-X系马氏体相变的热力学[J].金属学报,1980,16(04):420-4,25. |
[25] | Dai Q X;Yang R Z .The calculation of Tδand Vδin austenitic steel[J].Mater Charac,1997,38(03):129-133. |
[26] | Q.X. Dai;X.N. Cheng;Y.T. Zhao .Design of martensite transformation temperature by calculation for austenitic steels[J].Materials Characterization,2004(4/5):349-354. |