通过测定负极放电电流、放电电位、极化曲线和析氢速率研究添加镁对锂负极在碱性水溶液中放电性能和析氢反应行为的影响.结果表明,在锂中添加0.07%Mg(质量分数)降低了锂负极的析氢速率.锂镁合金负极电流效率比纯锂负极高,放电电流密度略低于纯锂负极,高电流密度放电时放电电位比纯锂负极略有正移.极化曲线测量结果表明,Li-0.07%Mg(质量分数)合金负极开路电位比纯锂负极稍有正移,自腐蚀微电池电流密度接近纯锂负极.XRD结果表明,锂镁合金负极放电后表面膜主要由LiOH、LiOH·H2O和Mg(OH)2组成.SEM结果表明,锂镁合金负极放电后的表面膜比纯锂负极表面膜的孔隙少,即添加镁降低锂负极析氢速率与负极表面膜中形成的Mg(OH)2对提高膜的完整性有关.

参考文献

[1] 刘景东,王文继.金属-水固态贮备电池的研究[J].电池,2005(03):188-190.
[2] Flores J R .[D].Pennsylvania:Pennsylvania State University,1999.
[3] Littauer E L;Tsai K C .[J].Journal of the Electrochemical Society,1976,123(06):771.
[4] Littauer E L;Momyer W R;Tsai K.C .[J].Journal of Power Sources,1977,2(02):163.
[5] Littauer E L;Tsai K C .[J].Journal of the Electrochemical Society,1977,124:850.
[6] Littauer E L;Tsai K C;Hollandsworth R P .[J].Journal of the Electrochemical Society,1978,125(06):845.
[7] Littauer E L;Tsai K C .[J].Journal of the Electrochemical Society,1976,123(07):964.
[8] Littauer E L;Tsai K C .[J].Journal of the Electrochemical Society,1980,127(03):521.
[9] Urquidi-Macdonald M;Macdonald D D;Pensado-Rodriguez O et al.[J].Electrochimica Acta,2001,47:833.
[10] Pensado-Rodr'iguez O .[D].Pennsylvania:Pennsylvania State University,1998.
[11] Mima Urquidi-Macdonald;Jose' Flores R;Digby Macdonald D et al.[J].Electrochimica Acta,1998,43:3069.
[12] Tsai C et al.[P].U S Patent,3 976 509,1976.
[13] Pensado O;Urquidi-Macdonald M;Macdonald D D .[J].Journal of the Electrochemical Society,1999,146(04):1318.
[14] Pensado-Rodr'iguez O;Flores J R;Urquidi-Macdonald M et al.[J].Journal of the Electrochemical Society,1999,146(04):1326.
[15] Mirna Urquidi-Macdonald;Homero Castaneda;Angela M. Cannon .Lithium fuel cells - I: lithium/poly(organophosphazene) membrane anodes in KOH and seawater[J].Electrochimica Acta,2002(15):2495-2503.
[16] Yancheng Zhang;Mima Urquidi-Macdonald .[J].Journal of Power Sources,2004,129:312.
[17] Yancheng Zhang;Mirna Urquidi-Macdonald .[J].Journal of Power Sources,2005,144:191.
[18] Shuster N.[A].IEEE,1992:118.
[19] Shuster N .[P].US Patent,No.5,427,873,1995.
[20] Cho J J;Urquidi-Macdonald M.[A].Orlando:Walt Disney World Dolphin,2000
[21] Kashiwara Shin .[P].Japan Patent,No.57017565,1982.
[22] Herman Urbach Annapolis B;David Icenhower E;Glen Dale et al.[P].US Patent,No.3980498,1974.
[23] 丁飞,张晶,杨凯,王磊,易炜,刘兴江.金属锂电极在KOH碱性溶液中的腐蚀研究(Ⅰ)[J].电源技术,2008(02):91-94.
[24] 丁飞,张晶,杨凯,王磊,易炜,刘兴江.金属锂电极在KOH碱性溶液中的腐蚀研究(Ⅱ)[J].电源技术,2008(04):247-248.
[25] 杨宏孝;凌芝;颜秀茹.无机化学[M].北京:高等教育出版社,2002:287.
[26] Nayeb-Hashemi A A;Pelton A D;Clark J B.二元合金相图[M].北京:高等教育出版社,1984:1487.
[27] 付承华 .[D].Wuhan:Huazhong University of Science&Technology,2005.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%