首次采用含镍硅酸乙酯(NiTEOS)进行溶胶-凝胶反应来制备高镍含量的Ni/SiO2复合气凝胶,且Ni含量可在<60wt%的范围内任意调节.并系统研究了水浓度、催化剂浓度、溶剂用量及合镍硅酸乙酯的组成对溶胶-凝胶过程的影响.所制备的Ni/SiO2复合气凝胶的比表面积高达420~650m2/g.
Ni-rich Ni/SiO2 composite aerogels in which weight percentage of Ni could reach 60% werefirstly prepared by sol-gel process of Ni-containing tetraethyl orthosilicate (NiTEOS). The influenceof H2O, catalyst, solvent and compostcomposition of Ni-containing tetraethyl orthosilicate on the sol-gelprocess was discussed. The specific sufrace areas of Ni/SiO2 composite aerogels are in the rangeof 420~650m2/g.