通过对工业纯镁以及ZM21合金的性能测试研究了镁合金在可降解生物医学中的应用,讨论了等径角挤压制备超细晶以及温挤压对材料性能的影响.晶粒细化导致合金材料压缩强度明显提高,强烈的初始变形织构导致粗晶镁合金拉伸强度高于压缩.等径角挤压能够减弱织构的影响,使不同合金塑性流变行为获得改变.材料腐蚀性能主要受化学成分、晶粒大小以及先前变形诱导晶格畸变程度的综合影响.等径角挤压细化晶粒、增大晶格缺陷密度在一定程度上制衡了材料的腐蚀性能.同时弥散分布的第二相粒子的增加对于点蚀发展有着积极的作用.

参考文献

[1] Schinhammer M;Hanzi AC;Loffler JF;Uggowitzer PJ .Design strategy for biodegradable Fe-based alloys for medical applications.[J].Acta biomaterialia,2010(5):1705-1713.
[2] Hermawan H;Dube D;Mantovani D .Developments in metallic biodegradable stents.[J].Acta biomaterialia,2010(5):1693-1697.
[3] Liu B;Zheng YF .Effects of alloying elements (Mn, Co, Al, W, Sn, B, C and S) on biodegradability and in vitro biocompatibility of pure iron.[J].Acta biomaterialia,2011(3):1407-1420.
[4] Hort N;Huang Y;Fechner D;Stormer M;Blawert C;Witte F;Vogt C;Drucker H;Willumeit R;Kainer KU;Feyerabend F .Magnesium alloys as implant materials--principles of property design for Mg-RE alloys.[J].Acta biomaterialia,2010(5):1714-1725.
[5] Ge,Q.;Dellasega,D.;Demir,A.G.;Vedani,M. .The processing of ultrafine-grained Mg tubes for biodegradable stents[J].Acta biomaterialia,2013(10):8604-8610.