欢迎登录材料期刊网

材料期刊网

高级检索

对Fe-Al金属间化合物的高温力学性能和抗氧化性能的研究现状进行了回顾.归纳和描述了固溶强化、析出强化、有序强化、弥散强化等强化机理以及Fe-Al材料抗氧化的机理.并对Fe-Al材料研究的发展进行了展望.

参考文献

[1] Stoloff N S .[J].Materials Science and Engineering,1998,A258:1.
[2] Liu C T;George E P;Maziasz P J et al.[J].Materials Science and Engineering,1998,A258:84.
[3] 张永刚.[M].北京:国防工业出版社,2001
[4] 汤文明,唐红军,郑治祥,吴玉程,董季玲.Fe-Al金属间化合物强韧化研究进展[J].合肥工业大学学报(自然科学版),2005(02):129-134.
[5] Palm M .[J].Intermetallics,2005,13:1286.
[6] Risanti D D;Sauthoff G .[J].Intermetallics,2005,13:1313.
[7] Stein F;Palm M;Sauthoff G .[J].Intermetallics,2005,13:1275.
[8] Morris D G et al.[J].Acta Materialia,2006,54:2335.
[9] Morris D G et al.[J].Acta Mater,2004,52:2827.
[10] Morris D G;Requejo L M et al.[J].Intermetallics,2005,13:862.
[11] Herrmann J;Inden G;Sauthoff G .[J].Steel Research International,2004,75:343.
[12] Baligidad R G;Prakash U .Krishna A Radha[J].Materials Science and Engineering,1997,A230:188.
[13] Schneider A;Falat L;Sauthoff G et al.[J].Intermetallics,2005,13:1322.
[14] Stallybrass C;Schneider A;Sauthoff G .[J].Intermetallics,2005,13:1263.
[15] Anthony L;Fultz B .[J].Aeta Metall Mater,1995,43:3885.
[16] Ohnuma I;Schon C G;Kainuma R et al.[J].Acta Materialia,1998,46:2083.
[17] Palm M;Sauthoff G .[J].Intermetallics,2004,12:1345.
[18] 姚正军,苏宏华,向定汉.合金元素的添加对Fe3Al基合金有序转变温度的影响[J].南京航空航天大学学报,2002(03):230-234.
[19] 周瑞发;韩雅芳;李树索.高温结构材料[M].北京:国防工业出版社,2006
[20] Schneider A;Falat L;Sauthoff G et al.[J].Intermetallics,2003,11:443.
[21] Falat L;Schneider A;Sauthoff G et al.[J].Intermetallics,2005,13:1256.
[22] Munoz-Morris M A;Garcia C;Morris D G .[J].Acta Materialia,2002,50:2825.
[23] Doucakis T;Kumar K S .[J].INTERMETALLICS,1999,7:765.
[24] Park B G;Ko S H;Park Y H et al.[J].Intermetallics,2006,14:660.
[25] Grosdidier T;Suzon E;Wagner F .[J].Intermetallics,2004,12:645.
[26] Kobayashi Satoru .[J].Zaefferer StefarL Intermetallics,2006,14:1252.
[27] Zhu Su-Ming;Tamura Makoto;Sakamoto Kazushi et al.[J].Mater Sei Eng,2000,A292:83.
[28] 唐红军,汤文明,郑治祥,吴玉程.机械合金化合成Fe-Al系纳米材料研究进展[J].材料导报,2004(z1):25-28.
[29] Minay E J .[J].Journal of Materials Processing Technology,2004,153-154(1-3):630.
[30] 尹衍升;李嘉 等.[J].粉末冶金技术,2004,22(31):51.
[31] Krasnowski M .[J].INTERMETALLICS,2007,15(02):201.
[32] Charlot F.;Gaffet E.;Klein D.;Niepce JC.;Bernard F. .In situ time-resolved diffraction coupled with a thermal IR camera to study mechanically activated SHS reaction: Case of Fe-Al binary system[J].Acta materialia,1999(2):619-629.
[33] Paris S;Gaffet E;Bernard F et al.[J].Scripta Materialia,2004,50:691.
[34] 陈君平 .[J].机械工程材料,2005,29(10):51.
[35] 李嘉,尹衍升,郝春成.纳米Fe3Al粉体及块体材料的制备及表征[J].机械工程学报,2005(03):81-85.
[36] Grosdidier Thierry;Ji Gang;Bernard Frederic et al.[J].Intermetallics,2006,14(10-11):1208.
[37] Morris D G.[J].Materials Science and Engineering A:Structural Materials:Properties Microstructure and Processing,2006(10):083.
[38] Malek P;Kratoehvil P;Pesicka J et al.[J].Intermetallics,2002,10:985.
[39] Krarochvil P;Pesicka J;Hakl J et al.[J].Journal of Alloys and Compounds,2004,378:258.
[40] Eumann M;Palm M;Sauthoff G .[J].Intermetallics,2004,12:625.
[41] Zhang W J;Sundar R S;Deevi S C .[J].Intermetallics,2004,12:893.
[42] Kratochvil P et al.[J].INTERMETALLICS,2007,15(03):333.
[43] Sundar R S;Deeri S C .[J].Materials Science and Engineering,2003,A357:124.
[44] Morris D G;Munoz-Morris M A .[J].Intermetallics,2005,13:1269.
[45] Kupka Marian .[J].Intermetallies,2006,14:149.
[46] 孙扬善;余新泉;黄海波 等.[J].金属学报,1998,34(11):1131.
[47] Tortorelli P F;Natesan K .[J].Materials Science and Engineering,1998,A258:115.
[48] Grabke H J .[J].INTERMETALLICS,1999,7:1153.
[49] 牛焱,侯嫣.高温氧化时Al2O3/FeAl界面孔洞形成过程的分析[J].金属学报,2003(10):1065-1070.
[50] Wright I G;Pint B A .[J].Oxidation of Metals,2001,55(3-4):333.
[51] Montealegre M A et al.[J].Intermetallics,2000,8:439.
[52] Lang Fengqun;Yu Zhiming;Gedevanishvili Shalva et al.[J].Intermetaltics,2004,12:451.
[53] 郦定强.钛对FeAl金属间化合物高温氧化行为的影响[J].材料工程,1998(09):14.
[54] Shankar Rao V .[J].Materials Science and Engineering,2004,A364:232.
[55] 王永刚,何业东,朱日彰.微晶Fe3Al高温氧化动力学研究[J].应用科学学报,1999(01):119-121.
[56] Pedraza F;Grosseau-Poussard J L;Dinhut J F .[J].Intermetallics,2005,13:27.
[57] 王永刚,何业东,朱日彰.电沉积-热解Y2O3薄膜提高Fe3Al高温氧化膜的保护性[J].中国稀土学报,1998(03):226-229.
[58] Juzon P et al.[J].Applied Surface Science,2006,252:5384.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%