利用FLOW-3D软件,对某本体铸件生产过程中出现的缩孔及疏松缺陷进行了模拟。模拟结果显示,在缺陷一侧增加浇口,同时对各浇冒口横截面及距离进行相应调整,缩孔及疏松缺陷消除。验证结果表明,根据模拟结果对石膏型低压铸造工艺进行优化后,试制的某本体铸件未见缩孔及疏松等铸造缺陷。
The shrinkage defects of body casting during practical production were simulated by FLOW-3D software. The results show that the shrinkage defects are eliminated effectively by adding a gate on one side of casting defects,and at the same time making the corresponding adjustment to the riser size and distance. The production practice indicates that the plaster casting process can be optimized by computer simulation,which can conveniently and quickly solve the problems of casting.
参考文献
[1] | 刘致远.铸造CAE技术的应用[J].中国铸造装备与技术,2003(06):26-29. |
[2] | 黄晓.客车后桥壳铸件工艺数值模拟及优化设计[J].汽车科技,2003(04):9-11. |
[3] | 米国发,和双双.飞轮铸件铸造工艺过程的数值模拟与工艺改进[J].航天制造技术,2008(03):26-30. |
[4] | 张可锋,杨涤心,谢敬佩,王爱琴,王文焱,李洛利.大型挂舵臂铸钢件铸造工艺优化[J].热加工工艺,2007(21):52-55. |
[5] | 米国发,何斌锋.计算机模拟在铸钢后桥工艺优化中的应用[J].航天制造技术,2008(02):44-48. |
[6] | 米国发,王锦永,王强,张锦志.圆锥破碎机传动轴架的铸造工艺设计及模拟优化[J].热加工工艺,2010(01):40-43. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%