离子注入对金属腐蚀行为的研究已达30年,研究结果表明离子注入对改变金属表面成分和表面性能是极为有效的技术,本文概述了离子注入对铁及其低合金、铝及其合金的腐蚀电化学行为的影响,涉及的注入离子达十余种.

参考文献

[1] 李青.离子注入技术及离子注入对不锈钢腐蚀电化学行为的影响[J].功能材料,2003(05):496-499,504.
[2] Ensinger W .[J].Electrochimica Acta,1994,39:1.
[3] Rangel C M;Paiva T I C .[J].Surface and Coatings Technology,1996,83:194.
[4] Nielsen B R et al.[J].Instrumentation and Methods,1991,B59/60:772.
[5] Singh A et al.[J].Corrosion,1990,46:367.
[6] Chenghui X et al.[J].Journal of Materials Science Letters,1996,15:245.
[7] JIN H et al.[J].Corrosion,1997,53:730.
[8] Zhang X L et al.[J].Materials Science,1999,34:159.
[9] Tian W et al.[J].Materials Science and Engineering,1989,A116:15.
[10] Wang S Y et al.[J].Instrumentation and Methods,1997,B127-128:1000.
[11] Zhang T H et al.[J].Surface and Coatings Technology,1996,83:280.
[12] Liang H et al.[J].Surface and Coatings Technology,2000,131:58.
[13] Granata R D et al.[J].Industrial and Engineering Chemistry Research,1987,26:427.
[14] Was G S et al.[J].Surface and Coatings Technology,1994,66:446.
[15] Sartwell B D et al.[J].Surface and Coatings Technology,1996,83:183.
[16] Wang P et al.[J].Instrumentation and Methods,1991,62:234.
[17] Lin W L et al.[J].Materials Science and Engineering,1997,B45:45.
[18] Tonghe Z et al.[J].中国科学E辑,1999,E42:623.
[19] McCafferty E et al.[J].Corrosion Science,1990,30:209.
[20] Yan P .[J].Applied Surface Science,1992,55:187.
[21] Li Y et al.[J].Surface and Coatings Technology,2000,128-129:205.
[22] Zhang X et al.[J].Instrumentation and Methods,2000,B169:112.
[23] Liang H et al.[J].Surface and Coatings Technology,2000,128-129:209.
[24] Iwaki M et al.[J].Surface and Coatings Technology,1992,51:1.
[25] Vollmer D P et al.[J].Analytical Letters,1997,30:359.
[26] Kim H J et al.[J].Materials Science and Engineering,1985,69:297.
[27] Tonghe Z et al.[J].Surface and Coatings Technology,2000,128-129:181.
[28] Wang W et al.[J].Surface and Coatings Technology,1999,111:97.
[29] Weber T et al.[J].Materials Science and Engineering,1995,A199:205.
[30] Wang S Y et al.[J].THIN SOLID FILMS,1997,311:190.
[31] Braun M et al.[J].Instrumentation and Methods,1989,B39:556.
[32] Braun M;er al .[J].Instrumentation and Methods,1987,B19-20:259.
[33] Leaven L van et al.[J].Surface and Coatings Technology,1992,53:25.
[34] Ueda Y et al.[J].Instrumentation and Methods,1993,B80/81:217.
[35] Sekiguchi A et al.[J].Surface and Coatings Technology,1992,51:13.
[36] Lillard R S et al.[J].Surface Engineering,1999,15:221.
[37] Bai X D et al.[J].Instrumentation and Methods,1995,B103:440.
[38] Pavlov P V et al.[J].Protection of Metals,1987,23:471.
[39] Sorensen N R et al.[J].Corrosion,1984,40:550.
[40] Fujihana T et al.[J].Surface and Coatings Technology,1992,51:19.
[41] Williams J M et al.[J].Instrumentation and Methods,1991,B59-60:845.
[42] Rangel C M et al.[J].Surface and Coatings Technology,1997,89:101.
[43] Smith P P et al.[J].Scripta Metallurgica et Materialia,1995,32:2021.
[44] Fernandes J C S.[J].Materials Science,1998:1151.
[45] Silva R C Da et al.[J].Instrumentation and Methods,1990,B50:423.
[46] Zhang X et al.[J].Corrosion Science,2001,43:85.
[47] Natishan P M et al.[J].Instrumentation and Methods,1991,B59/60:841.
[48] Emmerich R et al.[J].Surface and Coatings Technology,1994,66:436.
[49] McCafferty E. .Surface charge model of corrosion pit initiation and of protection by surface alloying[J].Journal of the Electrochemical Society,1999(8):2863-2869.
[50] Walter K C et al.[J].Instrumentation and Methods,1995,B106:522.
[51] Blawert C L et al.[J].Instrumentation and Methods,1997,B127-128:873.
[52] Massiani V et al.[J].Materials Science and Engineering,1987,A116:53.
[53] Matteson S et al.[J].Instrumentation and Methods,1985,B7/8:716.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%