在室温下的仿生溶液(FCS)中实现了钛合金表面的仿生矿化,得到羟基磷灰石(HA)涂层.跟踪分析了矿化过程中溶液pH值的变化,比较了矿化溶液中可能形成的各种磷酸钙陶瓷的过饱和度,发现HA的过饱和度最大,从而证明FCS溶液为HA涂层的形成提供了较好的热力学条件.

参考文献

[1] Silva PL.;Monteiro FJ.;Knowles JC.;Santos JD. .Adhesion and microstructural characterization of plasma-sprayed hydroxyapatite/glass ceramic coatings onto Ti-6A1-4V substrates[J].Surface & Coatings Technology,1998(3):191-196.
[2] Ding S J;Ju C P;Chern Lin J H .Morphology and Immer-sion Behavior of Plasma-sprayed Hydroxyapatite/bioacti-ve Glass Coatings[J].Journal of Materials Science:Materials in Medicine,2000,11(03):183-190.
[3] 王迎军;宁成云;赵子衷 et al.Changes of Bioactive Gradient Coatings in the Process of Plasma-spraying[J].中国陶瓷,1998,34(02):1-4.
[4] 程逵;翁文剑;葛曼珍 .Bioactive Ceramic Coatings[J].材料科学与工程,1998,16(03):8-12.
[5] Shirkhanzadeh M. .Nanoporous alkoxy-derived titanium oxide coating: a reactive overlayer for functionalizing titanium surface[J].Journal of Materials Science. Materials in Medicine,1998(6):355-362.
[6] 张玉梅,郭天文,李佐臣.牙用Ti-75合金铸造性能研究[J].稀有金属材料与工程,1999(02):125-128.
[7] 梁芳慧,周廉.钛和钛合金生物活化研究现状[J].稀有金属材料与工程,2003(04):241-245.
[8] 付涛,徐可为.仿生法沉积磷灰石层的研究进展[J].生物医学工程学杂志,2001(01):116-118.
[9] Li Tuantuan;Lee Junhee;Takayuki Kobayashi et al.Hyd-roxyapatite Coating by Dipping Method and Bone Bonding Strength[J].Journal of Materials Science:Materials in Medicine,1996,7(06):355-357.
[10] 邝志清,潘春跃,黄可龙,高鸿儒.Sol-gel法制备羟基磷酸钙超细粉末[J].中南工业大学学报,2000(03):246.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%