本文首次采用Czochralski法生长优质的Scx:Fey:Cuz:LN (x=0,1%, 2%, 3%, 3.5%, y=0.1%, z=0.06%)晶体.测试了晶体抗光致散射能力,以二波耦合光路测试晶体的衍射效率、写入时间和擦除时间,计算光折变灵敏度和动态范围.结果表明:Sc(2mol%):Fe:Cu:LN和Sc(3mol%):Fe:Cu:LN晶体抗光致散射能力比Fe:Cu:LN晶体高两个数量级以上,Scx:Fey:Cuz:LN晶体的写入速度、光折变灵敏度和动态范围等全息存储性能优于Fe:LN晶体.首次采用氪离子激光(482.0 nm,蓝光)作开关光,氦氖激光(632.8 nm,红光)做记录光,以Sc:Fe:Cu:LN晶体作为双光子全息存储记录介质,实现了双光子全息存储固定(非挥发性全息存储).

参考文献

[1] Buse k;Jermann F;kratizig E .Two-step Photorefractive Hologram Recording in LiNbO3:Fe[J].Ferroelectrics,1993,141(02):197-205.
[2] Youwen Liu;Liren Liu;De'an Liu;Liangying Xu;Changhe Zhou .Intensity dependence of two-center nonvolatile holographic recording in LiNbO_(3):Cu:Ce crystals[J].Optics Communications: A Journal Devoted to the Rapid Publication of Short Contributions in the Field of Optics and Interaction of Light with Matter,2001(1/6):339-343.
[3] Joyce K;Yamamoto;Kitamura K .Increased Optical Damage Resistance in Sc2O3-doped LiNbO3[J].Applied Physics Letters,1992,61(18):2156-2158.
[4] Buse K.;Adibi A.;Psaltis D. .Non-volatile holographic storage in doubly doped lithium niobate crystals[J].Nature,1998(6686):665-668.
[5] 赵朝中,周玉祥,张建,荣宪伟,徐玉恒.Zn:Fe:LiNbO3晶体的生长及其光学性能的研究[J].人工晶体学报,2004(02):184-188.
[6] 李铭华,赵业权,许克彬,徐玉恒,韩爱珍.氧化和还原处理对Fe:LiNbO3晶体光折变效应的影响[J].科学通报,1995(21):1955-1957.
[7] 王锐,徐衍岭,韦永德,赵朝中.Mg2+对Fe∶LiNbO3晶体光折变响应时间的影响[J].光子学报,2001(11):1307-1309.
[8] 周玉祥,郑威,刘彩霞,刘波,徐玉恒.Mg:Fe:LiNbO3晶体的生长及光学性能研究[J].光子学报,2004(05):577-580.
[9] 郭亚军,张建,刘彩霞,刘波,徐玉恒.Zn:Fe:LiNbO3晶体全息存储性能研究[J].光子学报,2004(05):570-572.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%