总结了近年来超细WC-Co硬质合金注射成形在原料粉末、粘结剂体系、混炼、注射成形、粘结剂脱除和烧结等方面的研究现状.讨论了不同脱脂方式的发展及其对碳含量的影响,重点阐述了控制晶粒长大、尺寸精度等关键技术存在的困难及解决途径.展望了超细WC-Co硬质合金注射成形技术的发展前景.

参考文献

[1] 陈振华,姜勇,陈鼎,张忠健,徐涛,彭文.硬质合金的疲劳与断裂[J].中国有色金属学报,2011(10):2394-2401.
[2] Qu Xuanhui;Gao Jianxiang;Qin Mingli et al.Application of a wax-based binder in PIM of WC-TiC-Co cemented carbides[J].Int Refract Metals Hard Mater,2005,23:273.
[3] 李志希,范景莲,黄伯云,成会朝.超细WC-Co硬质合金注射成形技术的研究现状[J].粉末冶金工业,2004(03):23-28.
[4] Matula G .Carbide alloyed composite manufactured with the powder injection moulding method and sinterhardened[J].Achievements Mater Manuf Eng,2010,42(1-2):164.
[5] Golombek K;Matula G;Mikula J et al.Influence of binder composition on the properties of feedstock for cemented carbides[J].Archives Mater Sci Eng,2011,51(02):116.
[6] Yang M J;German R M .Nanophase and super fine cemented carbides processed by powder injection molding[J].Int Refract Metals Hard Mater,1998,16(01):107.
[7] Lin S T;German R M .Extraction debinding of injection molded parts by condensed solvent[J].Powder Metallurgy International,1989,21(05):19.
[8] Martyn M T;James P J .The processing of hardmetal components by powder injection moulding[J].Int Refract Metals Hard Mater,1994,12(02):61.
[9] M. Youseffi;I. A. Menzies .Injection moulding of WC-6Co powder using two new binder systems based on montanester waxes and water soluble gelling polymers[J].Powder Metallurgy,1997(1):62-65.
[10] 祝宝军,曲选辉,陶颖.粉末注射成形热塑-热固粘结剂的开发研制[J].硬质合金,2003(03):149-153.
[11] 李志希 .硬质合金注射成形工艺的研究[D].中南大学,2005.
[12] Quinard C;Barriere T;Gelin J C .Development and property identification of 316L stainless steel feedstock for PIM and μPIM[J].Powder Technology,2009,190:123.
[13] Hunt K N;Evans J R G .The influence of mixing route on the properties of ceramic injection moulding blends[J].British Ceramic Transactions,1988,87:17.
[14] 祝宝军,曲选辉,王全亮.硬质合金注射成形工艺进展[J].湖南有色金属,2001(06):35-39.
[15] 李昆,李晓明,李笃信,赵利刚,李益民,黄伯云.表面活性剂对MIM硬质合金粘结剂和喂料性质的影响[J].材料科学与工程,2002(02):248-250.
[16] Mutsuddy B C .Study of ceramic injection molding parameters[J].Advanced Ceramic Materials,1987,2:213.
[17] 祝宝军,曲选辉,陶颖,肖平安,秦明礼.硬质合金注射成形注射参数的优化[J].稀有金属材料与工程,2002(03):232-235.
[18] 李志希,范景莲,刘涛,肖琼.硬质合金注射工艺参数的研究[J].硬质合金,2005(01):32-35.
[19] 范景莲,廖雪松,成会朝,刘涛,田家敏."一步热脱脂+烧结"工艺对注射成形硬质合金显微结构与性能的影响[J].稀有金属材料与工程,2008(12):2236-2239.
[20] 祝宝军,曲选辉,陶颖,肖平安,秦明礼.YG8硬质合金的粉末注射成形技术[J].粉末冶金材料科学与工程,2002(03):247-252.
[21] Mahmoodan M;Aliakbarzadeh H;gholamipour R .Sintering of WC-10%Co nano powders containing TaC and VC grain growth inhibitors[J].Transactions of Nonferrous Metals Society of China,2011,21:1080.
[22] Hayashi K;Fuke Y;Suzuki H .Effects of additional carbides on the grain size of WC-Co alloys[J].Journal of the Japan Society of Powder and Powder Metallurgy,1972,19:67.
[23] PANG Cholsong,LUO Ji,GUO Zhimeng.Microstructure and properties of ultrafine WC-10Co composites with chemically doped VC[J].稀有金属(英文版),2011(02):183-188.
[24] 孙兰 .超细WC-Co硬质合金制备及WC晶粒长大研究[D].北京科技大学,2008.
[25] Suzuki K;Fuke Y;Hayashi K .Grain size of WC in sintered WC-VC-Co alloys[J].Journal of the Japan Society of Powder and Powder Metallurgy,1972,19:106.
[26] Johnny Bruhn;Bjorn Terselius .MIM offers increased applications for submicron WC-10%Co: Seco Tools is looking at the application of MIM for cutting tools using submicron WC-10%Co hardmetal[J].Metal Powder Report,1999(1):30-33.
[27] Choi S H;Kang S D;Kwon Y S et al.The effect of sintering conditions on the properties of WC-10wt%Co PIM compacts[J].Research on Chemical Intermediates,2010,36:743.
[28] Giles G;Szesny B;Dreyer K et al.Submicron and ultrafine grained hardmetals for microdrills and metal cutting inserts[J].Int Refract Metals Hard Mater,2002,20:3.
[29] Randall M. German .Wear applications offer further growth for PIM[J].Metal Powder Report,1999(6):24-28.
[30] 祝宝军 .硬质合金注射成形工艺研究[D].中南大学,2002.
[31] German R M;宋久鹏.粉末注射成形——材料、性能、设计与应用[M].北京:机械工业出版社,2011:1.