以工业碱木质素为原料,变压油为分散相,添加分散剂十二烷基硫酸钠及交联剂环氧氯丙烷,采用"反相悬浮聚合法"制备出球形多孔木质素珠体.通过单因素及正交试验筛选制备木质素多孔珠体的影响因素并对球形木质素珠体进行了形貌、红外光谱、X衍射分析.结果分析表明,制备木质素珠体的最佳配比为:5g木质素溶于50mL水中,pH值为10~13,分散剂0.2g,交联剂3g,变压油150mL,制备的木质素珠体产率达到87.75%,有效粒径在0.6~1.4mm之间.珠体的形貌分析表明木质素珠体球形度好,具有微孔结构;红外光谱分析表明木质素与环氧氯丙烷发生了交联反应;X衍射分析表明交联的木质素珠体仍是无定形高分子.
参考文献
[1] | Bonini C.;D'auria M.;Ferri R.;Pucciariello R.;Sabia AR. .Graft copolymers of lignin with electron poor alkenes[J].Journal of Applied Polymer Science,2003(4):1163-1171. |
[2] | Wu Yun;Zhang Shuzhen;Guo Xueyan et al.[J].Bioresource Technology,2008,99:7709-7715. |
[3] | Meister J J .[J].Journal of Macromol Sci Polymer Reviews,2002,42(02):235-289. |
[4] | Guo Xueyan;Zhang Shuzhen;Shan Xiaoquan .[J].Journal of Hazardous Materials B:Environmental Technologies,2008,151:134-142. |
[5] | Kadla J F;Kubo S;Venditti R A et al.[J].Journal of Applied Polymer Science,2002,85:1353-1355. |
[6] | 范娟 .多功能球形木质素基吸附材料的制备及其性能研究[D].华南理工大学,2005. |
[7] | Baklanova O N;Plaksin G V;Drozdov V A et al.[J].CARBO,2003,41:1793-1800. |
[8] | Suhas;Carrott PJM;Carrott MMLR .Lignin - from natural adsorbent to activated carbon: A review[J].Bioresource Technology: Biomass, Bioenergy, Biowastes, Conversion Technologies, Biotransformations, Production Technologies,2007(12):2301-2312. |
[9] | Harmita, H;Karthikeyan, KG;Pan, XJ .Copper and cadmium sorption onto kraft and organosolv lignins[J].Bioresource Technology: Biomass, Bioenergy, Biowastes, Conversion Technologies, Biotransformations, Production Technologies,2009(24):6183-6191. |
[10] | 洪树楠 .一种球形木质素金属吸附剂的研制及其应用研究[D].福州:福州大学,2002. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%