高级检索

以甲基丙烯酸甲酯和含氟丙烯酸酯为接枝单体制备了改性三元乙丙橡胶(MEPDM)和氟橡胶(FPM)/MEPDM反应型并用胶.利用全反射傅立叶变换红外光谱仪(ATR-FT-IR)、橡胶硫化分析仪(ODR)、动态热机械分析(DMA)和扫描电镜(SEM)等研究了FPM/MEPDM并用胶的结构与性能,同时考察了材料老化前后的力学性能.结果表明,改性单体的接枝率为28.03%,接枝效率为58.54%;并用胶可以实现共硫化,硫化胶界面结合紧密;硫化胶的综合性能随着FPM用量的增大而提高,且老化后力学性能有所改善,含氟官能团向材料表面迁移.

参考文献

[1] Kader MA.;Bhowmick AK. .Acrylic rubber-fluorocarbon rubber miscible blends: Effect of curatives and fillers on cure, mechanical, aging, and swelling properties[J].Journal of Applied Polymer Science,2003(5):1442-1452.
[2] Bernard Boutevin;Gerardo Caporiccio;Francine Guida-Pietrasanta;Amedee Ratsimihety .Poly-silafluoroalkyleneoligosiloxanes:a class of fluoroelastomers with low glass transition temperature[J].Journal of Fluorine Chemistry,2003(2):131-138.
[3] Hirano K;Suzuki K;Nakano K;Tosaka M .Phase separation structure in the polymer blend of fluorocarbon elastomer and hydrogenated nitrile rubber[J].Journal of Applied Polymer Science,2005(1):149-156.
[4] 黄月文,刘伟区,罗广建,寇勇.含氟丙烯酸酯-苯乙烯共聚物的制备及其表面性能的研究[J].功能高分子学报,2005(02):269-273.