The effect of different decomposition conditions on tungsten recovery for scheelite concentrate has been examined. The results show that tungsten recovery can be more than 98% under decomposing conditions as follows: the amount of caustic soda is 2.2 and 3.2 times of theoretical respectively, ratio of water and ore is 0.7-0.8, temperature is 160℃, and preservation time is 2.0 h for scheelite concentrate (63.21% WO3) and low grade scheelite concentrate (55.17% WO3).

参考文献

[1] Li H G;Sun P.M;Li Y.J.Facing challenge of industry, improving our tungsten hydrometallurgy technique to emulate the top countries[J].China Tungsten Industry(in Chinese),2001(5-6):49-51.
[2] Li H G.Rare metals metallurgy (in Chinese)[M].北京:冶金工业出版社,1990
[3] Li H G;Liu M.H;Si Z.J et al.Caustic Decomposition to Scheelite Concentrate and Scheelite-wolframite Mixed Concentrate: Technique and Equipmen[P].Chinese Patent, 85 1 00350.8,1985.
[4] Li H G;Liu M.H;Dai C.J.Research to new technique of tungsten caustic decomposition[J].Rare Metals and Cemented Carbides(in Chinese),1987(1-2):1.
[5] Li Y J;Sun P.M;Liu M.S et al.Mechanical activated caustic decomposition to scheelite concentrate[J].Transactions of Nonferrous Metals Society of China,1995,5(03):27.
[6] Liu M S;Sun P.M;Li Y.J et al.Mechanical activated caustic decomposition of tungsten concentrate with a high content of calcium[M].ICHM'92,1:296.
[7] Zelikmann A H.Metallurgy of Rare Metals[M].Metall; Mosco,1991:33.
[8] Li H G.Foundation and New Technique of Tungsten Caustic Decomposition (in Chinese)[M].Central South University of Technology Publisher,Changsha,1997:1-10.
[9] Sun P M;Li Y.J;Li H.G.Energetics of scheelite caustic decomposition[J].Transactions of Nonferrous Metals Society of China,1993(02):37.