欢迎登录材料期刊网

材料期刊网

高级检索

针对用于ITER(International Thermonuclear Experimental Reactor)的316L(N)型奥氏体不锈钢,研究分析了其中形成的σ相的特征、相形成过程、检测方法以及对性能的影响,以加深基础研究工作者和工程技术人员对σ相的了解,促进316L(N)生产工艺的完善和产品质量的进一步提高.结合相关研究的最新进展,展望了今后的研究及发展趋势.

参考文献

[1] Lo K H;Shek C H;Lai J K L .Recent Developments in Stainless Steels[J].Materials Science and Engineering:Reports,2009,65:39.
[2] Treitschke W;Tammann G .Enthalpy of Formation for σ-Phase Solid Solutions at 1060K[J].Z Anorg Chem,1907,55:402.
[3] Bain E C;Griffiths W E .An Introduction to the Iron-Chromium Nickel Alloys[J].Trans AIME,1927,75:166.
[4] Lai J K L .A Review of Precipitation Behavior in AISI Type 316 Stainless Steel[J].Material Science and Engineering,1983,61:101.
[5] Bergmann G;Shoemaker D R .The Determination of the Crystal Structure of the σ-Phase in the Iron-Chromium and IronMolybdenum Systems[J].Acta Crystallographica,1954,7:857.
[6] Andrews K W;Dyson D J;Keown S R.Interpretation of Electron Diffraction Patterns[M].London:Adam Hilger,1967
[7] Ohmura T;Tsuzaki K;Sawada K et al.Inhomogeneous NanoMechanical Properties in the Multi-Phase Microstructure of Long-Term Aged Type 316 Stainless Steel[J].Journal of Materials Research,2006,21(06):1229.
[8] Ohmura, T;Sawada, K;Kimura, K;Tsuzaki, K .Alteration in nanohardness of matrix phase associated with precipitation during long-term aging of type 316 stainless steel[J].Materials Science and Engineering. A, Structural Materials: Properties, Microstructure and Processing,2008(1/2):85-92.
[9] Michael Pohl;Oliver Storz;Thomas Glogowski .Effect of intermetallic precipitations on the properties of duplex stainless steel[J].Materials Characterization,2007(1):65-71.
[10] Read D A;Thomas E H .Evidence of Itinerant Electron Ferromagnetism in Sigma Phase Alloys[J].Journal of Physics and Chemistry of Solids,1968,29(09):1569.
[11] M. Gich;E. A. Shafranovsky;A. Roig;A. Slawska-Waniewska;K. Racka;LI. Casas;Yu. I. Petrov;E. Molins;M. F. Thomas .Aerosol nanoparticles in the Fe_(1-x)Cr_x system: Room-temperature stabilization of the σ phase and σ → α-phase transformation[J].Journal of Applied Physics,2005(2):024303.1-024303.8.
[12] Lai J K L;Shek C H;Wong K W .Review of Temperature Indicators and the Use of Duplex Stainless Steels for Life Assessment[J].Materials Science and Engineering:Reports,1997,19(5/6):153.
[13] Lai J K L;Wong K W;Li D J .Effect of Solution Treatment on the Transformation Behaviour of Cold-Rolled Duplex Stainless Steels[J].Materials Science and Engineering A,1995,2003(1/2):356.
[14] Gupta K P;Rajan N S;Beck P A .Effect of Si and Al on the Stability of Certain Sigma Phases[J].Transactions of the Metallurgical Society of AIME,1960,218:617.
[15] Bergman B G;Shoemaker D P .The Determination of the Crystal Structure of the Phase in the Iron-Chromium and Iron-Molybdenum Systems[J].Acta Crystallographica,1954,7(12):857.
[16] Weiss B;Stickler R .Phase Instabilities During High Temperature Exposure of 316 Austenitic Stainless Steel[J].Metallurgical Transactions,1972,3(04):851.
[17] Kuo K .Carbides in Chromium,Molybdenum and Tungsten Steels[J].J Iron Steel Inst,1953,173(04):363.
[18] Koutsky J;Jezek J .High-Temperature Properties of 12Cr Steels Alloyed With Tungsten,Molybdenum and Vanadium[J].J Iron Steel Inst,1965,203:707.
[19] Hsaio C M;Dulis E J .Effect of Interstitial Carbon Plus Nitrogen and Precipitation Reactions on the Properties of Austenitic Cr-Mn-C-N Steels[J].Trans ASM,1960,52:855.
[20] Singhal L K;Martin J W .The Formation of Ferrite and Sigma-Phase in Some Austenitic Stainless Steels[J].ACTA METALLURGICA,1968,16(12):1441.
[21] Woodyatt L R;Sims C T;Beattie H J .Prediction of SigmaType Phase Occurrence From Compositions in Austemtic Superalloys[J].Transactions of the Metallurgical Society of ALME,1966,236:519.
[22] Villanueva D M E;Junior F C P;Plaut R L et al.Comparative Study on Sigma Phase Precipitation of Three Types of Stainless Steels:Austenite,Superferritic and Duplex[J].Materials Science and Technology,2006,22(09):1098.
[23] Padilha AF;Escriba DM;Materna-Morris E;Rieth M;Klimenkov M .Precipitation in AISI 316L(N) during creep tests at 550 and 600 degrees C up to 10 years[J].Journal of Nuclear Materials: Materials Aspects of Fission and Fusion,2007(1):132-138.
[24] Bhamjia I;Preussa M;Threadgillb P L et al.Linear Friction Welding of AISI 316L Stainless Steel[J].Materials Science and Engineering A,2010,528:680.
[25] Ghosh Chowdhury S;Mukhopadhyay N K;Das G et al.Failure Analysis of a Weld Repaired Steam Turbine Casing[J].Eng Failure Anal,1998,5:205.
[26] Parnian N .Failure Analysis of Austenitic Stainless Steel Tubes in a Gas Fired Steam Heater[J].Materials and Design,2012,36:788.
[27] Lai J K L .A Study of Precipitation in AISI Type 316 Stainless Steel[J].Material Science and Engineering,1983,58(02):195.
[28] Small M;Ryba E .Calculation and Evaluation of the Gibbs Energies of Formation of Cr3C2,Cr7C3,and Cr23C6[J].Metallurgical Transactions,1981,12(08):1389.
[29] Chastell D J;Flewitt P E J .The Formation of the Sigma Phase During Long Term High Temperature Creep of Type 316 Austenitic Stainless Steel[J].Material Science and Engineering,1979,38:153.
[30] Pardal J M;Carvalho S S;Barbosa C et al.Failure Analysis of AISI 310S Plate in an Inert Gas Generator Used in Off-Shore Oil Platform[J].ENGINEERING FAILURE ANALYSIS,2011,18:1435.
[31] Roychowdhury S;Kain V;Matcheswala A et al.Sigma-Phase Induced Embrittlement in Titanium Containing Austenitic Stainless Steel Tie-Bars in a Condenser[J].ENGINEERING FAILURE ANALYSIS,2012,25:123.
[32] Totten G E.Steel Heat Treatment Handbook[M].Boca Raton,USA:CRC Press,2007
[33] Terada M;Escriba D M;Costa I et al.Investigation on the Intergranular Corrosion Resistance of the AISI 316L (N)Stainless Steel After Long Time Creep Testing at 600 ℃[J].Materials Characterization,2008,59:663.
[34] Lai J K L;Wickens A .Microstructural Changes and Variations in Creep Ductility of 3 Casts of Type 316 Stainless Steel[J].Acta Metall,1979,27:217.
[35] Muhammad Farooq;Rolf Sandstrom;Mats Lundberg .Precipitation during long time ageing in the austenitic stainless steel 310[J].Materials at High Temperatures,2012(1):8-16.
[36] Conejero O;Palacios M;Rivera S .Premature Corrosion Failure of a 316L Stainless Steel Plate due to the Presence of Sigma Phase[J].ENGINEERING FAILURE ANALYSIS,2009,16:699.
[37] Schwind M;Kallqvist J;Nilsson J-O et al.Sigma-Phase Precipitation in Stabilized Austenitic Stainless Steels[J].Acta Materilia,2000,48:2473.
[38] Vach M;Kuníková T;Dománková M et al.Evolution of Secondary Phases in Austenitic Stainless Steels During LongTerm Exposures at 600,650 and 800 ℃[J].Materials Characterization,2008,59:1792.
[39] Weiss B;Hughes C W;Stickler R .Scanning-Electron-Microscope Techniques for the Micro-Characterization of Metals and Alloys[J].Praktische Metallographie,1971,8:528.